Solution-processed negative gauge factor PtSe2 strain sensors
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60461373%3A22310%2F25%3A43932180" target="_blank" >RIV/60461373:22310/25:43932180 - isvavai.cz</a>
Výsledek na webu
<a href="https://pubs.rsc.org/en/content/articlehtml/2025/nr/d5nr01217a" target="_blank" >https://pubs.rsc.org/en/content/articlehtml/2025/nr/d5nr01217a</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1039/d5nr01217a" target="_blank" >10.1039/d5nr01217a</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Solution-processed negative gauge factor PtSe2 strain sensors
Popis výsledku v původním jazyce
We undertake electrochemical exfoliation of a 2D semiconductor platinum diselenide, PtSe2 and investigate the piezoresistance response of a solution-processed network. Due to the large PtSe2 aspect ratios, exceeding 300, we achieve conformal flake-to-flake junctions and good inter-flake electrical coupling. Our measured piezoresistive gauge factor is negative (-5.45), consistent with the intrinsic negative gauge factor of PtSe2. This negative network gauge factor implies that strain is transferred from the substrate to the nanosheets. However, detailed modelling shows that the strain transferred to the nanosheets is much smaller than the applied strain, showing that conformal junctions do not necessarily lead to good mechanical coupling between nanosheets. Our model implies that this gauge factor is consistent with a strain transfer efficiency of 8.5%. Our strain sensor also demonstrated a cyclic response for over 1000 cycles, enabling the sensor to be used in future flexible optoelectronics applications.
Název v anglickém jazyce
Solution-processed negative gauge factor PtSe2 strain sensors
Popis výsledku anglicky
We undertake electrochemical exfoliation of a 2D semiconductor platinum diselenide, PtSe2 and investigate the piezoresistance response of a solution-processed network. Due to the large PtSe2 aspect ratios, exceeding 300, we achieve conformal flake-to-flake junctions and good inter-flake electrical coupling. Our measured piezoresistive gauge factor is negative (-5.45), consistent with the intrinsic negative gauge factor of PtSe2. This negative network gauge factor implies that strain is transferred from the substrate to the nanosheets. However, detailed modelling shows that the strain transferred to the nanosheets is much smaller than the applied strain, showing that conformal junctions do not necessarily lead to good mechanical coupling between nanosheets. Our model implies that this gauge factor is consistent with a strain transfer efficiency of 8.5%. Our strain sensor also demonstrated a cyclic response for over 1000 cycles, enabling the sensor to be used in future flexible optoelectronics applications.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
10402 - Inorganic and nuclear chemistry
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2025
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Nanoscale
ISSN
2040-3364
e-ISSN
2040-3372
Svazek periodika
17
Číslo periodika v rámci svazku
8th July 2025
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
9
Strana od-do
18083-18091
Kód UT WoS článku
001532390900001
EID výsledku v databázi Scopus
—