Tepelná kapacita, entalpie a entropie strontium bismut niobátu a strontium bismut tantalátu
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60461373%3A22340%2F06%3A00016715" target="_blank" >RIV/60461373:22340/06:00016715 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Heat capacity, enthalpy and entropy of strontium bismuth niobate and strontium bismuth tantalate
Popis výsledku v původním jazyce
The heat capacities and enthalpy increments of strontium bismuth niobate SrBi2Nb2O9 (SBN) and strontium bismuth tantalate SrBi2Ta2O9 (SBT) were measured by the relaxation method (2-150 K), Calvet-type heat-conduction calorimetry (305-570 K) and drop calorimetry (773-1373 K). The temperature dependences of non-transition heat capacities in the form Cpm = 324.47 + 0.06371T - 5.0755 x 106/T2 J K-1 mol-1 (298-1400 K) and Cpm = 320.22 + 0.06451T - 4.7001 x 106/T2 J K-1 mol-1 (298-1400 K) were derived for SBNand SBT, respectively, by the least-squares method from the experimental data. Furthermore, the standard molar entropies at 298.15 K Sm[deg](SBN)=327.15+/-0.80 and Sm[deg](SBT)=339.23+/-0.72 J K-1 mol-1 were evaluated from the low-temperature heat capacity measurements.
Název v anglickém jazyce
Heat capacity, enthalpy and entropy of strontium bismuth niobate and strontium bismuth tantalate
Popis výsledku anglicky
The heat capacities and enthalpy increments of strontium bismuth niobate SrBi2Nb2O9 (SBN) and strontium bismuth tantalate SrBi2Ta2O9 (SBT) were measured by the relaxation method (2-150 K), Calvet-type heat-conduction calorimetry (305-570 K) and drop calorimetry (773-1373 K). The temperature dependences of non-transition heat capacities in the form Cpm = 324.47 + 0.06371T - 5.0755 x 106/T2 J K-1 mol-1 (298-1400 K) and Cpm = 320.22 + 0.06451T - 4.7001 x 106/T2 J K-1 mol-1 (298-1400 K) were derived for SBNand SBT, respectively, by the least-squares method from the experimental data. Furthermore, the standard molar entropies at 298.15 K Sm[deg](SBN)=327.15+/-0.80 and Sm[deg](SBT)=339.23+/-0.72 J K-1 mol-1 were evaluated from the low-temperature heat capacity measurements.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
CF - Fyzikální chemie a teoretická chemie
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2006
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Thermochimica Acta
ISSN
0040-6031
e-ISSN
—
Svazek periodika
450
Číslo periodika v rámci svazku
1-2
Stát vydavatele periodika
NL - Nizozemsko
Počet stran výsledku
5
Strana od-do
105-109