Dynamics of N2 and N2O Peaks During and After the Regeneration of Lean NOx Trap
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60461373%3A22340%2F15%3A43900071" target="_blank" >RIV/60461373:22340/15:43900071 - isvavai.cz</a>
Výsledek na webu
<a href="http://www.sciencedirect.com/science/article/pii/S0926337314007747" target="_blank" >http://www.sciencedirect.com/science/article/pii/S0926337314007747</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.apcatb.2014.12.002" target="_blank" >10.1016/j.apcatb.2014.12.002</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Dynamics of N2 and N2O Peaks During and After the Regeneration of Lean NOx Trap
Popis výsledku v původním jazyce
The dynamics and selectivity of N2 and N2O formation during and after the regeneration of a commercial NOx storage catalyst containing Pt, Pd, Rh, Ba on Ce/Zr, Mg/Al and Al oxides was studied with high-speed FTIR and SpaciMS analyzers. The lean/rich cycling experiments (60 s/5 s and 60 s/3 s) were performed in the temperature range 200-400 oC, using H2, CO, and C3H6 individually for the reduction of adsorbed NOx. Isotopically labeled 15NO was employed in combination with Ar carrier gas in order to quantify the N2 product by mass spectrometry. N2 and N2O products were formed concurrently. The primary peaks appeared immediately after the rich-phase inception, and tailed off with breakthrough of the reductant front (accompanied by NH3 product). SecondaryN2 and N2O peaks appeared at the rich-to-lean transition as a result of reactions between surface-deposited reductants/intermediates (CO, HC, NH3, -NCO) and residual stored NOx. At 200-300 oC, up to 30% of N2 and 50% of N2O products origi
Název v anglickém jazyce
Dynamics of N2 and N2O Peaks During and After the Regeneration of Lean NOx Trap
Popis výsledku anglicky
The dynamics and selectivity of N2 and N2O formation during and after the regeneration of a commercial NOx storage catalyst containing Pt, Pd, Rh, Ba on Ce/Zr, Mg/Al and Al oxides was studied with high-speed FTIR and SpaciMS analyzers. The lean/rich cycling experiments (60 s/5 s and 60 s/3 s) were performed in the temperature range 200-400 oC, using H2, CO, and C3H6 individually for the reduction of adsorbed NOx. Isotopically labeled 15NO was employed in combination with Ar carrier gas in order to quantify the N2 product by mass spectrometry. N2 and N2O products were formed concurrently. The primary peaks appeared immediately after the rich-phase inception, and tailed off with breakthrough of the reductant front (accompanied by NH3 product). SecondaryN2 and N2O peaks appeared at the rich-to-lean transition as a result of reactions between surface-deposited reductants/intermediates (CO, HC, NH3, -NCO) and residual stored NOx. At 200-300 oC, up to 30% of N2 and 50% of N2O products origi
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
CI - Průmyslová chemie a chemické inženýrství
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/LH12086" target="_blank" >LH12086: Analýza, modelování a řízení časoprostorových koncentračních profilů v katalyzátorech pro redukci oxidů dusíku (deNOx) v automobilových výfukových plynech</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2015
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Applied Catalysis B:Environment
ISSN
0926-3373
e-ISSN
—
Svazek periodika
166-167
Číslo periodika v rámci svazku
neuveden
Stát vydavatele periodika
BE - Belgické království
Počet stran výsledku
9
Strana od-do
509-517
Kód UT WoS článku
—
EID výsledku v databázi Scopus
—