Equilibrium sorption of ethylene in polyethylene: Experimental study and PC-SAFT simulations
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F60461373%3A22340%2F15%3A43900606" target="_blank" >RIV/60461373:22340/15:43900606 - isvavai.cz</a>
Výsledek na webu
<a href="http://www.sciencedirect.com/science/article/pii/S0032386115000518" target="_blank" >http://www.sciencedirect.com/science/article/pii/S0032386115000518</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.polymer.2015.01.012" target="_blank" >10.1016/j.polymer.2015.01.012</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Equilibrium sorption of ethylene in polyethylene: Experimental study and PC-SAFT simulations
Popis výsledku v původním jazyce
Ethylene sorption in polyethylene (PE) influences the reaction rate in polymerization reactors and the subsequent degassing of residual monomer. The knowledge of ethylene solubilities is therefore important for process design and optimization. We used agravimetric apparatus based on a magnetic suspension balance to measure ethylene solubilities in 13 PE samples at temperatures from 60 to 150 oC. The samples were nascent reactor powders with densities from 902 to 967 kg mMINUS SIGN 3 and weight averagemolecular weights from 98 to 253 kg molMINUS SIGN 1. The experimental data were compared with the literature and the entire data set was correlated using the PC-SAFT equation of state. To evaluate the solubilities, we used swelling corrections based on experimental data and considered temperature dependent crystallinities. As a result, the ethylene solubilities decreased with increasing temperature and increasing PE crystallinity. Furthermore, we observed a temperature independent PC-SAF
Název v anglickém jazyce
Equilibrium sorption of ethylene in polyethylene: Experimental study and PC-SAFT simulations
Popis výsledku anglicky
Ethylene sorption in polyethylene (PE) influences the reaction rate in polymerization reactors and the subsequent degassing of residual monomer. The knowledge of ethylene solubilities is therefore important for process design and optimization. We used agravimetric apparatus based on a magnetic suspension balance to measure ethylene solubilities in 13 PE samples at temperatures from 60 to 150 oC. The samples were nascent reactor powders with densities from 902 to 967 kg mMINUS SIGN 3 and weight averagemolecular weights from 98 to 253 kg molMINUS SIGN 1. The experimental data were compared with the literature and the entire data set was correlated using the PC-SAFT equation of state. To evaluate the solubilities, we used swelling corrections based on experimental data and considered temperature dependent crystallinities. As a result, the ethylene solubilities decreased with increasing temperature and increasing PE crystallinity. Furthermore, we observed a temperature independent PC-SAF
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
CI - Průmyslová chemie a chemické inženýrství
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GAP106%2F10%2F1912" target="_blank" >GAP106/10/1912: Morfologií ovlivněná sorpce a difuze penetrantů v polymerech</a><br>
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2015
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Polymer
ISSN
0032-3861
e-ISSN
—
Svazek periodika
59
Číslo periodika v rámci svazku
neuveden
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
8
Strana od-do
270-277