Tenké mesoporézní filmy ZnO připravené elektrodepozicí jako účinné fotokatalyzátory pro degradaci polutantů barviv
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61388955%3A_____%2F07%3A00087868" target="_blank" >RIV/61388955:_____/07:00087868 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Electrodeposited Mesoporous ZnO Thin Films as Efficient Photocatalysts for the degradation of dye pollutants
Popis výsledku v původním jazyce
Thin mesoporous films of ZnO were prepared by electrochemical deposition using eosin Y as a structure-directing agent. After removal of the eosin from the structure, transparent porous ZnO films were obtained. The porosity and surface area of these filmswere determined by performing krypton BET measurements. Electrochemical deposition parameters, such as the deposition time and the eosin concentration in the plating bath, were optimized to prepare films with large internal surface areas and good mechanical properties. Eosin concentrations of 50-60 M were found to give the best-quality mesoporous zinc oxide films with film thicknesses ranging from 2 to 3 m. The photodegradations of a heteropolyaromatic dye (methylene blue) and a diazo dye (congo red) served as model reactions to assess the photocatalytic activity of the zinc oxide films. For both dyes, the photodegradation rate reached its maximum for mesoporous films that were prepared with eosin concentrations above 40 M.
Název v anglickém jazyce
Electrodeposited Mesoporous ZnO Thin Films as Efficient Photocatalysts for the degradation of dye pollutants
Popis výsledku anglicky
Thin mesoporous films of ZnO were prepared by electrochemical deposition using eosin Y as a structure-directing agent. After removal of the eosin from the structure, transparent porous ZnO films were obtained. The porosity and surface area of these filmswere determined by performing krypton BET measurements. Electrochemical deposition parameters, such as the deposition time and the eosin concentration in the plating bath, were optimized to prepare films with large internal surface areas and good mechanical properties. Eosin concentrations of 50-60 M were found to give the best-quality mesoporous zinc oxide films with film thicknesses ranging from 2 to 3 m. The photodegradations of a heteropolyaromatic dye (methylene blue) and a diazo dye (congo red) served as model reactions to assess the photocatalytic activity of the zinc oxide films. For both dyes, the photodegradation rate reached its maximum for mesoporous films that were prepared with eosin concentrations above 40 M.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
CF - Fyzikální chemie a teoretická chemie
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2007
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Journal of Physical Chemistry C
ISSN
1932-7447
e-ISSN
—
Svazek periodika
111
Číslo periodika v rámci svazku
21
Stát vydavatele periodika
US - Spojené státy americké
Počet stran výsledku
6
Strana od-do
7639-7644