Purification of a conducting polymer, polyaniline, for biomedical applications
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61389013%3A_____%2F14%3A00429814" target="_blank" >RIV/61389013:_____/14:00429814 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/70883521:28610/14:43871796
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.synthmet.2014.06.020" target="_blank" >http://dx.doi.org/10.1016/j.synthmet.2014.06.020</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.synthmet.2014.06.020" target="_blank" >10.1016/j.synthmet.2014.06.020</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Purification of a conducting polymer, polyaniline, for biomedical applications
Popis výsledku v původním jazyce
A conducting polymer, polyaniline, was prepared in globular and nanotubular morphologies. The protonated forms were converted to the corresponding bases and both types of samples were tested for cytotoxicity. The polyanilines were then suspended in N-methylpyrrolidone or in concentrated sulphuric acid, and the soluble parts were precipitated into methanol acidified with sulphuric acid. Such a dissolution/precipitation cycle was tested as a purification procedure for polyaniline, which would remove the potential low-molecular-weight components. The original morphology of polyaniline was destroyed in soluble part (18?24 wt.%) but maintained in the fraction insoluble in N-methylpyrrolidone. The fraction soluble in sulphuric acid was higher (56?64 wt.%). The original morphology converted to fragments after reprecipitation, and the samples became amorphous. The conductivity was reduced on average by two orders of magnitude. FTIR spectroscopy was used to assess the molecular structure, hydro
Název v anglickém jazyce
Purification of a conducting polymer, polyaniline, for biomedical applications
Popis výsledku anglicky
A conducting polymer, polyaniline, was prepared in globular and nanotubular morphologies. The protonated forms were converted to the corresponding bases and both types of samples were tested for cytotoxicity. The polyanilines were then suspended in N-methylpyrrolidone or in concentrated sulphuric acid, and the soluble parts were precipitated into methanol acidified with sulphuric acid. Such a dissolution/precipitation cycle was tested as a purification procedure for polyaniline, which would remove the potential low-molecular-weight components. The original morphology of polyaniline was destroyed in soluble part (18?24 wt.%) but maintained in the fraction insoluble in N-methylpyrrolidone. The fraction soluble in sulphuric acid was higher (56?64 wt.%). The original morphology converted to fragments after reprecipitation, and the samples became amorphous. The conductivity was reduced on average by two orders of magnitude. FTIR spectroscopy was used to assess the molecular structure, hydro
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
CD - Makromolekulární chemie
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GA13-08944S" target="_blank" >GA13-08944S: Vodivé polymery a jejich interakce s buňkami.</a><br>
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2014
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Synthetic Metals
ISSN
0379-6779
e-ISSN
—
Svazek periodika
195
Číslo periodika v rámci svazku
September
Stát vydavatele periodika
CH - Švýcarská konfederace
Počet stran výsledku
8
Strana od-do
286-293
Kód UT WoS článku
000341469300040
EID výsledku v databázi Scopus
—