Microstructure and sliding wear properties of HVOF sprayed, laser remelted and laser clad Stellite 6 coatings
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61389021%3A_____%2F17%3A00476973" target="_blank" >RIV/61389021:_____/17:00476973 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/49777513:23640/17:43932090
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.surfcoat.2016.09.012" target="_blank" >http://dx.doi.org/10.1016/j.surfcoat.2016.09.012</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.surfcoat.2016.09.012" target="_blank" >10.1016/j.surfcoat.2016.09.012</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Microstructure and sliding wear properties of HVOF sprayed, laser remelted and laser clad Stellite 6 coatings
Popis výsledku v původním jazyce
The microstructure and sliding wear properties of Co-Cr-W alloy (Stellite 6) coatings were studied in the dependence on the deposition technology. The HVOF as-sprayed, laser remelted HVOF sprayed and laser clad coatings were evaluated by SEM, XRD and ASTM G-133 reciprocating sliding wear test. In dependence on used deposition technology, the microstructure of coating varied namely in terms of grain size and phase composition. The XRD analyses in the wear track revealed that the strain-induced fcc-to-hcp transformation is taking part during wear of laser remelted HVOF sprayed coatings. The difference of the phase composition, grain size and strain-induced fcc-to-hcp transformation was shown to be responsible for differences in the sliding wear behaviour.
Název v anglickém jazyce
Microstructure and sliding wear properties of HVOF sprayed, laser remelted and laser clad Stellite 6 coatings
Popis výsledku anglicky
The microstructure and sliding wear properties of Co-Cr-W alloy (Stellite 6) coatings were studied in the dependence on the deposition technology. The HVOF as-sprayed, laser remelted HVOF sprayed and laser clad coatings were evaluated by SEM, XRD and ASTM G-133 reciprocating sliding wear test. In dependence on used deposition technology, the microstructure of coating varied namely in terms of grain size and phase composition. The XRD analyses in the wear track revealed that the strain-induced fcc-to-hcp transformation is taking part during wear of laser remelted HVOF sprayed coatings. The difference of the phase composition, grain size and strain-induced fcc-to-hcp transformation was shown to be responsible for differences in the sliding wear behaviour.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20506 - Coating and films
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2017
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Surface and Coatings Technology
ISSN
0257-8972
e-ISSN
—
Svazek periodika
318
Číslo periodika v rámci svazku
May
Stát vydavatele periodika
CH - Švýcarská konfederace
Počet stran výsledku
13
Strana od-do
129-141
Kód UT WoS článku
000402356100016
EID výsledku v databázi Scopus
2-s2.0-84994525007