CORROSION OF DRY - BOTTOM BOILER EVAPORATOR IN POWER INDUSTRY
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27230%2F15%3A86095946" target="_blank" >RIV/61989100:27230/15:86095946 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.4028/www.scientific.net/MSF.818.129" target="_blank" >http://dx.doi.org/10.4028/www.scientific.net/MSF.818.129</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.4028/www.scientific.net/MSF.818.129" target="_blank" >10.4028/www.scientific.net/MSF.818.129</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
CORROSION OF DRY - BOTTOM BOILER EVAPORATOR IN POWER INDUSTRY
Popis výsledku v původním jazyce
This contribution solves the character of corrosive damage of the tubes, steam generating tubes of dry-bottom boiler combustion chamber in power plant engineering, and deals with the aspects related to the corrosion criteria of the carbon steel. The laboratory test results of samples applied on tubes that were subject to non-destructive and destructive tests are analyzed in one part of the work. The samples of greater incidence of corrosion products, which caused the failure of the integrity of the steam generating tubes, were tested. The contribution deals in details with the results of laboratory and chemical analysis of boiler water from the previous periods. The article evaluates the amount and frequency of P2O5 dosing cycles. The work also deals with the proposal of corrective measures that shall lead to the chemical balance of the boiler water. It proposes a continuous correlation methodology for chemical stabilization.
Název v anglickém jazyce
CORROSION OF DRY - BOTTOM BOILER EVAPORATOR IN POWER INDUSTRY
Popis výsledku anglicky
This contribution solves the character of corrosive damage of the tubes, steam generating tubes of dry-bottom boiler combustion chamber in power plant engineering, and deals with the aspects related to the corrosion criteria of the carbon steel. The laboratory test results of samples applied on tubes that were subject to non-destructive and destructive tests are analyzed in one part of the work. The samples of greater incidence of corrosion products, which caused the failure of the integrity of the steam generating tubes, were tested. The contribution deals in details with the results of laboratory and chemical analysis of boiler water from the previous periods. The article evaluates the amount and frequency of P2O5 dosing cycles. The work also deals with the proposal of corrective measures that shall lead to the chemical balance of the boiler water. It proposes a continuous correlation methodology for chemical stabilization.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JK - Koroze a povrchové úpravy materiálu
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/ED3.1.00%2F14.0320" target="_blank" >ED3.1.00/14.0320: Pre-seed aktivity VŠB-TUO II - Materiály</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2015
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Materials Science Forum
ISSN
1662-9752
e-ISSN
—
Svazek periodika
818
Číslo periodika v rámci svazku
May 2015
Stát vydavatele periodika
CH - Švýcarská konfederace
Počet stran výsledku
4
Strana od-do
129-132