Impact assessment of input factors on tool electrode wear in die sinking EDM of Steel EN43CrMo4
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27230%2F17%3A10236104" target="_blank" >RIV/61989100:27230/17:10236104 - isvavai.cz</a>
Výsledek na webu
<a href="https://www.scopus.com/record/display.uri?eid=2-s2.0-85029948430&origin=resultslist&sort=plf-f&src=s&sid=736777873d9fd2ac461eaed9c576ffc9&sot=autdocs&sdt=autdocs&sl=18&s=AU-ID%2857189048724%29&relpos=1&citeCnt=0&searchTerm=" target="_blank" >https://www.scopus.com/record/display.uri?eid=2-s2.0-85029948430&origin=resultslist&sort=plf-f&src=s&sid=736777873d9fd2ac461eaed9c576ffc9&sot=autdocs&sdt=autdocs&sl=18&s=AU-ID%2857189048724%29&relpos=1&citeCnt=0&searchTerm=</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.4028/www.scientific.net/KEM.756.127" target="_blank" >10.4028/www.scientific.net/KEM.756.127</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Impact assessment of input factors on tool electrode wear in die sinking EDM of Steel EN43CrMo4
Popis výsledku v původním jazyce
The paper deals with the wear of tool electrodes for Die Sinking EDM. In the experiment were used the electrodes of copper and graphite. The workpiece material was steel EN43CrMo4. For the assessment the effects of each parameter was used the statistical method Design of Experiments (DOE). Assessed input factors were the peak current, pulse on-time, pulse off-time, and the electrode material. The result of the effects of each input factors was tool electrode wear. For calculating the relative wear of electrodes was used the percentage of the ratio of the electrode and the workpiece weight. The results show that the expression of the relative wear in practice can be described as a method unusable due to the absorption of the graphite electrode used in the experiment. © 2017 Trans Tech Publications, Switzerland.
Název v anglickém jazyce
Impact assessment of input factors on tool electrode wear in die sinking EDM of Steel EN43CrMo4
Popis výsledku anglicky
The paper deals with the wear of tool electrodes for Die Sinking EDM. In the experiment were used the electrodes of copper and graphite. The workpiece material was steel EN43CrMo4. For the assessment the effects of each parameter was used the statistical method Design of Experiments (DOE). Assessed input factors were the peak current, pulse on-time, pulse off-time, and the electrode material. The result of the effects of each input factors was tool electrode wear. For calculating the relative wear of electrodes was used the percentage of the ratio of the electrode and the workpiece weight. The results show that the expression of the relative wear in practice can be described as a method unusable due to the absorption of the graphite electrode used in the experiment. © 2017 Trans Tech Publications, Switzerland.
Klasifikace
Druh
J<sub>SC</sub> - Článek v periodiku v databázi SCOPUS
CEP obor
—
OECD FORD obor
20301 - Mechanical engineering
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2017
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Materials Structure & Micromechanics of Fracture
ISSN
1013-9826
e-ISSN
—
Svazek periodika
756
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
US - Spojené státy americké
Počet stran výsledku
9
Strana od-do
127-135