Initial Yield Locus Tracking for Stainless Steel Produced by SLM Technology
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27230%2F22%3A10260069" target="_blank" >RIV/61989100:27230/22:10260069 - isvavai.cz</a>
Výsledek na webu
<a href="http://experimentalni-mechanika.cz/cs/konference/konference/2022/file/2998-1411_prispevek.html" target="_blank" >http://experimentalni-mechanika.cz/cs/konference/konference/2022/file/2998-1411_prispevek.html</a>
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Initial Yield Locus Tracking for Stainless Steel Produced by SLM Technology
Popis výsledku v původním jazyce
The study of initial anisotropy is done for 316L stainless steel produced by 3D printing. A non-destructive tracing method is used to determine the initial yield locus. Experiments were performed in two printing directions and three loading paths were tested. The specimens were loaded proportionally and a combination of axial and torsional loading was used. The yield stress is defined as the deviation from the linearity. The resulting dispersion between the probing paths is negligible. The direction of printing affects the shape of the initial yield locus. For the horizontally printed specimens, the points can be approximated according to the von-Mises criterion. For vertically printed specimens, the shear stress component was dominant, and the initial yield surface appears as an ellipse.
Název v anglickém jazyce
Initial Yield Locus Tracking for Stainless Steel Produced by SLM Technology
Popis výsledku anglicky
The study of initial anisotropy is done for 316L stainless steel produced by 3D printing. A non-destructive tracing method is used to determine the initial yield locus. Experiments were performed in two printing directions and three loading paths were tested. The specimens were loaded proportionally and a combination of axial and torsional loading was used. The yield stress is defined as the deviation from the linearity. The resulting dispersion between the probing paths is negligible. The direction of printing affects the shape of the initial yield locus. For the horizontally printed specimens, the points can be approximated according to the von-Mises criterion. For vertically printed specimens, the shear stress component was dominant, and the initial yield surface appears as an ellipse.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
—
OECD FORD obor
20302 - Applied mechanics
Návaznosti výsledku
Projekt
<a href="/cs/project/EF17_049%2F0008407" target="_blank" >EF17_049/0008407: Inovativní a aditivní technologie výroby - nová technologická řešení 3D tisku kovů a kompozitních materiálů</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2022
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Ean 2022 Proceedings of the 60th Annual Conference on Experimental Stress Analysis
ISBN
978-80-01-07400-8
ISSN
—
e-ISSN
—
Počet stran výsledku
4
Strana od-do
198-201
Název nakladatele
České Vysoké Učení Technické v Praze
Místo vydání
Praha
Místo konání akce
Praha
Datum konání akce
6. 6. 2022
Typ akce podle státní příslušnosti
EUR - Evropská akce
Kód UT WoS článku
—