Monitoring conductivity and optical homogeneity during the growth of PANI thin films
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27240%2F13%3A86086149" target="_blank" >RIV/61989100:27240/13:86086149 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/61989100:27640/13:86086149
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.tsf.2013.04.048" target="_blank" >http://dx.doi.org/10.1016/j.tsf.2013.04.048</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.tsf.2013.04.048" target="_blank" >10.1016/j.tsf.2013.04.048</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Monitoring conductivity and optical homogeneity during the growth of PANI thin films
Popis výsledku v původním jazyce
In order to optimize the technology with respect to maximum conductivity, transmittance and optical homogeneity, the time-controlled chemical bath deposition process was used to prepare polyaniline (PANI) thin films on glass substrate. Two different precursors have been used for PANI thin films preparation: anilinium sulfate and aniline hydrochloride. Optical homogeneity has been evaluated by transmittance maps obtained using spectrometer equipped with light collecting multi-mode optical fibers. Resultsshowed the strong dependence of conductivity and optical homogeneity on the deposition time during early stages of films growth. The increase of conductivity during deposition time is accompanied with the increase of optical inhomogeneity. Optimum deposition time has been estimated about 30 min with maximum optical homogeneity, keeping still the reasonable transmittance and conductivity values.
Název v anglickém jazyce
Monitoring conductivity and optical homogeneity during the growth of PANI thin films
Popis výsledku anglicky
In order to optimize the technology with respect to maximum conductivity, transmittance and optical homogeneity, the time-controlled chemical bath deposition process was used to prepare polyaniline (PANI) thin films on glass substrate. Two different precursors have been used for PANI thin films preparation: anilinium sulfate and aniline hydrochloride. Optical homogeneity has been evaluated by transmittance maps obtained using spectrometer equipped with light collecting multi-mode optical fibers. Resultsshowed the strong dependence of conductivity and optical homogeneity on the deposition time during early stages of films growth. The increase of conductivity during deposition time is accompanied with the increase of optical inhomogeneity. Optimum deposition time has been estimated about 30 min with maximum optical homogeneity, keeping still the reasonable transmittance and conductivity values.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JJ - Ostatní materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2013
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Thin Solid Films
ISSN
0040-6090
e-ISSN
—
Svazek periodika
537
Číslo periodika v rámci svazku
30. června 2013
Stát vydavatele periodika
NL - Nizozemsko
Počet stran výsledku
7
Strana od-do
58-64
Kód UT WoS článku
000319456400007
EID výsledku v databázi Scopus
—