Microstructure of Ti-46Al-5Nb-1W alloy after directional solidification
Popis výsledku v původním jazyce
Intermetallic alloys based on g-TiAl two-phases alloys are sought-after materials for assumed applications in aerospace and automotive industries. Their favorable properties, such as low density and good corrosion resistance, are accompanied on the otherhand by low toughness and very difficult metallurgy. One of the possibilities to improve the toughness of Ti-46Al-5Nb-1W (at.%) alloy consists in change of their microstructure into lamellar microstructure, which can be reached moreover by directional solidifcation. This experiment is described in this paper. Samples of the Ti-46Al-5Nb-1W (at.%) alloy were prepared by plasma melting. Then the samples were remelted in vacuum-induction furnace becouse of the low homogenity. Cast samples were subjected todirectional solidifcation. Cooling rates were constant and ranged from 20 mm/h to 425 mm/h. Directional solidification has been accomplished in ceramic tubes made of corundum - Al2O3. The samples were studied by metallographic analysis.
Název v anglickém jazyce
Microstructure of Ti-46Al-5Nb-1W alloy after directional solidification
Popis výsledku anglicky
Intermetallic alloys based on g-TiAl two-phases alloys are sought-after materials for assumed applications in aerospace and automotive industries. Their favorable properties, such as low density and good corrosion resistance, are accompanied on the otherhand by low toughness and very difficult metallurgy. One of the possibilities to improve the toughness of Ti-46Al-5Nb-1W (at.%) alloy consists in change of their microstructure into lamellar microstructure, which can be reached moreover by directional solidifcation. This experiment is described in this paper. Samples of the Ti-46Al-5Nb-1W (at.%) alloy were prepared by plasma melting. Then the samples were remelted in vacuum-induction furnace becouse of the low homogenity. Cast samples were subjected todirectional solidifcation. Cooling rates were constant and ranged from 20 mm/h to 425 mm/h. Directional solidification has been accomplished in ceramic tubes made of corundum - Al2O3. The samples were studied by metallographic analysis.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2006
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
13. Internationaler Studententag der Metallurgie
ISBN
3-901384-18-9
ISSN
—
e-ISSN
—
Počet stran výsledku
6
Strana od-do
189-195
Název nakladatele
ASMET, Austrian Society for Metallurgy and Materials
Místo vydání
Leoben
Místo konání akce
—
Datum konání akce
—
Typ akce podle státní příslušnosti
—
Kód UT WoS článku
—