Acicular ferrite and bainite fractal response
Popis výsledku v původním jazyce
The work deals with acicular ferrite (AF) and upper bainite (B) relations. Both austenite decomposition products are practically nucleated at the same temperature interval by displacive mechanism, only the formation positions are different. The AF comesinto existence at the specific particles intragranularly, while the B is intergranularly nucleated at the austenite grains. This leads to high strength properties of both products, however different toughness levels. The B impact toughness is unbalancedand reaches lower levels unlike the AF. The differences can be observed in fractal dimensions, too. The higher is the fractal dimension the more cleavage fracture can be awaited. This was also demonstrated in case of both austenite decomposition products. In the area of ductile fracture the determined fractal dimensions differences are small.
Název v anglickém jazyce
Acicular ferrite and bainite fractal response
Popis výsledku anglicky
The work deals with acicular ferrite (AF) and upper bainite (B) relations. Both austenite decomposition products are practically nucleated at the same temperature interval by displacive mechanism, only the formation positions are different. The AF comesinto existence at the specific particles intragranularly, while the B is intergranularly nucleated at the austenite grains. This leads to high strength properties of both products, however different toughness levels. The B impact toughness is unbalancedand reaches lower levels unlike the AF. The differences can be observed in fractal dimensions, too. The higher is the fractal dimension the more cleavage fracture can be awaited. This was also demonstrated in case of both austenite decomposition products. In the area of ductile fracture the determined fractal dimensions differences are small.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2009
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Hutnické listy
ISSN
0018-8069
e-ISSN
—
Svazek periodika
2009
Číslo periodika v rámci svazku
6
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
6
Strana od-do
—
Kód UT WoS článku
—
EID výsledku v databázi Scopus
—