Popis výsledku v původním jazyce
The knowledge of round blank temperature field during its casting and cooling makes possible to solve the problematic of inner structure, surface quality, blank mechanical properties, metallurgical length, casting crust thickness growth for different casting velocities and steel overheating. For each mould there is correlation between the thermal flow, which is removed from solidifying steel to cooling water, and temperature of the mould copper wall. From the temperature profile along the wall height orcircumference it can be deduced, how tight is the contact between the blank surface and the mould wall and thus what intensity and evenness of heat removal is in the place in question. The heat removal should be, as far as possible, constant in the mould location and even along the circumference of cross-section.
Název v anglickém jazyce
Heat transport in mould for continuous casting of steel
Popis výsledku anglicky
The knowledge of round blank temperature field during its casting and cooling makes possible to solve the problematic of inner structure, surface quality, blank mechanical properties, metallurgical length, casting crust thickness growth for different casting velocities and steel overheating. For each mould there is correlation between the thermal flow, which is removed from solidifying steel to cooling water, and temperature of the mould copper wall. From the temperature profile along the wall height orcircumference it can be deduced, how tight is the contact between the blank surface and the mould wall and thus what intensity and evenness of heat removal is in the place in question. The heat removal should be, as far as possible, constant in the mould location and even along the circumference of cross-section.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2010
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
METAL 2010
ISBN
978-80-87294-15-4
ISSN
—
e-ISSN
—
Počet stran výsledku
6
Strana od-do
—
Název nakladatele
TANGER s.r.o. Ostrava
Místo vydání
Rožnov pod Radhoštěm
Místo konání akce
Rožnov pod Radhoštěm
Datum konání akce
18. 5. 2010
Typ akce podle státní příslušnosti
EUR - Evropská akce
Kód UT WoS článku
—