Precipitation of ZnS nanoparticles and their deposition on montmorillonite
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27360%2F11%3A86080559" target="_blank" >RIV/61989100:27360/11:86080559 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1166/asem.2011.1087" target="_blank" >http://dx.doi.org/10.1166/asem.2011.1087</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1166/asem.2011.1087" target="_blank" >10.1166/asem.2011.1087</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Precipitation of ZnS nanoparticles and their deposition on montmorillonite
Popis výsledku v původním jazyce
ZnS nanoparticles were prepared by the precipitation of zinc acetate with sodium sulphide in aqueous solutions. The originated colloidal dispersions were stabilized by the cationic surfactant cetyltrimethylammonium (CTA). The ZnS nanoparticles size of 4nm was estimated from band-gap energies obtained from UV spectra. The nanoparticles were deposited on Na-rich montmorillonite (MMT). The size of created MMT agglomerates (ZnS-MMT-CTA) was measured by dynamic light scattering (DLS) method. The mean size of ZnS-MMT-CTA was about 300 nm and the total volume was about 38 vol.% higher than that of MMT. ZnS-MMT-CTA was dried at 105 oC and - 24 oC and studied by field emission electron microscopy (FESEM). Unlike the heated nanocomposite, the frozen one exhibited the porous structure.
Název v anglickém jazyce
Precipitation of ZnS nanoparticles and their deposition on montmorillonite
Popis výsledku anglicky
ZnS nanoparticles were prepared by the precipitation of zinc acetate with sodium sulphide in aqueous solutions. The originated colloidal dispersions were stabilized by the cationic surfactant cetyltrimethylammonium (CTA). The ZnS nanoparticles size of 4nm was estimated from band-gap energies obtained from UV spectra. The nanoparticles were deposited on Na-rich montmorillonite (MMT). The size of created MMT agglomerates (ZnS-MMT-CTA) was measured by dynamic light scattering (DLS) method. The mean size of ZnS-MMT-CTA was about 300 nm and the total volume was about 38 vol.% higher than that of MMT. ZnS-MMT-CTA was dried at 105 oC and - 24 oC and studied by field emission electron microscopy (FESEM). Unlike the heated nanocomposite, the frozen one exhibited the porous structure.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
CB - Analytická chemie, separace
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2011
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Advanced Science, Engineering and Medicine
ISSN
2164-6627
e-ISSN
—
Svazek periodika
3
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
US - Spojené státy americké
Počet stran výsledku
6
Strana od-do
113-118
Kód UT WoS článku
—
EID výsledku v databázi Scopus
—