Study of diamond-like coating deposited on the surface of Nd-Fe-B-TYPE sintered magnets
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27360%2F13%3A86088443" target="_blank" >RIV/61989100:27360/13:86088443 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Study of diamond-like coating deposited on the surface of Nd-Fe-B-TYPE sintered magnets
Popis výsledku v původním jazyce
Diamond-like coating (DLC) was deposited on ground and polished surfaces of Nd-Fe-B sintered magnet (prepared with 4 wt.% TbH2) using reactive ion-beam synthesis directly from ion-beam of a chemical complex substance (cyclohexane). The film deposited isdiamond-like; the fraction of tetragonal carbon-atom bonds is 70 %. The composition and thickness of the coating was analyzed by glow-discharge spectroscopy using a GDS 850A (LECO) spectrometer. The thickness of pure carbon (DLC) layer is 0.08 ?m. The existence of transition layer 0.08/0.07 ?m thick is due to the diffusion (to a lesser degree) and surface roughness. The effect of the coating of surface mechanical characteristics of the magnet was estimated in studying the Vickers hardness of the surfaceand friction coefficient and by nanoindentation as well. The Nd-Fe-B magnets with applied diamond-like coating demonstrate the lower tendency to mechanical cracking. Dry frictional tests showed that, after wear-in process, the DLC increa
Název v anglickém jazyce
Study of diamond-like coating deposited on the surface of Nd-Fe-B-TYPE sintered magnets
Popis výsledku anglicky
Diamond-like coating (DLC) was deposited on ground and polished surfaces of Nd-Fe-B sintered magnet (prepared with 4 wt.% TbH2) using reactive ion-beam synthesis directly from ion-beam of a chemical complex substance (cyclohexane). The film deposited isdiamond-like; the fraction of tetragonal carbon-atom bonds is 70 %. The composition and thickness of the coating was analyzed by glow-discharge spectroscopy using a GDS 850A (LECO) spectrometer. The thickness of pure carbon (DLC) layer is 0.08 ?m. The existence of transition layer 0.08/0.07 ?m thick is due to the diffusion (to a lesser degree) and surface roughness. The effect of the coating of surface mechanical characteristics of the magnet was estimated in studying the Vickers hardness of the surfaceand friction coefficient and by nanoindentation as well. The Nd-Fe-B magnets with applied diamond-like coating demonstrate the lower tendency to mechanical cracking. Dry frictional tests showed that, after wear-in process, the DLC increa
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/ED0040%2F01%2F01" target="_blank" >ED0040/01/01: Regionální materiálově technologické výzkumné centrum</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2013
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
METAL 2013 : 22nd International Conference on Metallurgy and Materials : conference proceedings : May 15th - 17th 2013, Hotel Voronez I, Brno Czech Republic, EU [CD-ROM]
ISBN
978-80-87294-41-3
ISSN
—
e-ISSN
—
Počet stran výsledku
6
Strana od-do
1358-1363