Evaluation of mechanical propertiesof the drawn wire using the design of experiments.
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27360%2F16%3A86098443" target="_blank" >RIV/61989100:27360/16:86098443 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Evaluation of mechanical propertiesof the drawn wire using the design of experiments.
Popis výsledku v původním jazyce
This paper deals with using the design of experiments (DOE) during the evaluation of mechanical properties of the wire for steel ropes. It was provided with a full factorial experiment with three factors at two levels. The factors are as follows: one-pass strain, the approaching angle and the method of the removing of the scales from the surface of hot rolled wire. The experimental material was a drawn wire with a 5.5 mm diameter of C78DP steel. The wire was drawn from the diameter of 5.5 mm to 2.5 mm using a straight-through single-block KOCH KGT 25 - E wire drawing machine. The total reduction was 79.3 %. The drawing dies of tungsten carbide had approach angles of 8o and 12o. Two uniform pass schedules were used with a different single-pass reduction. Two methods of descaling (mechanical and chemical) were used. Following each pass, an approx. 50 m sample was removed from the wire stock for subsequent testing. The following tests were carried out after each pass: tension test, torsion test to fracture and the reverse bend test to fracture. DOE was evaluated using both graphical and analytical methods. The significant factors and their interactions were determined and response surfaces were calculated.
Název v anglickém jazyce
Evaluation of mechanical propertiesof the drawn wire using the design of experiments.
Popis výsledku anglicky
This paper deals with using the design of experiments (DOE) during the evaluation of mechanical properties of the wire for steel ropes. It was provided with a full factorial experiment with three factors at two levels. The factors are as follows: one-pass strain, the approaching angle and the method of the removing of the scales from the surface of hot rolled wire. The experimental material was a drawn wire with a 5.5 mm diameter of C78DP steel. The wire was drawn from the diameter of 5.5 mm to 2.5 mm using a straight-through single-block KOCH KGT 25 - E wire drawing machine. The total reduction was 79.3 %. The drawing dies of tungsten carbide had approach angles of 8o and 12o. Two uniform pass schedules were used with a different single-pass reduction. Two methods of descaling (mechanical and chemical) were used. Following each pass, an approx. 50 m sample was removed from the wire stock for subsequent testing. The following tests were carried out after each pass: tension test, torsion test to fracture and the reverse bend test to fracture. DOE was evaluated using both graphical and analytical methods. The significant factors and their interactions were determined and response surfaces were calculated.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JS - Řízení spolehlivosti a kvality, zkušebnictví
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2016
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
METAL 2016: conference proceedings : (reviewed version) : 25th Anniversary International Conference on Metallurgy and Materials : May 25th-27th 2016, Hotel Voronez I, Brno, Czech Republic, EU
ISBN
978-80-87294-67-3
ISSN
—
e-ISSN
—
Počet stran výsledku
6
Strana od-do
501-506
Název nakladatele
Tanger
Místo vydání
Ostrava
Místo konání akce
Brno
Datum konání akce
25. 5. 2016
Typ akce podle státní příslušnosti
EUR - Evropská akce
Kód UT WoS článku
—