Study of kinetics phase transformations after plastic deformation of rail steel class IH alloyed with chromium
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27360%2F16%3A86099186" target="_blank" >RIV/61989100:27360/16:86099186 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Study of kinetics phase transformations after plastic deformation of rail steel class IH alloyed with chromium
Popis výsledku v původním jazyce
The paper is aimed at evaluation of effect previous plastic deformation on transformation kinetics of rail steel class IH alloyed with chromium. The CCT and DCCT diagrams were assembled on the basis of dilatometric tests with and/or without an influence of the previous deformation. To the experiment execution the dilation module of the plastometer Gleeble 3800 was used. The Accuracy of the diagrams was faced with metallographic analysis and measurement of hardness. The obtained results were compared with the results of in-process measurement of rail rolling mill Třinecké železárny Inc. This confirmed the theory that in the case of steels which are intended for rolling rails, no influence of the previous deformation the crucial influence pearlitic transformation in terms of time, but in the case of higher cooling rate has deformation an appreciable effect on shift temperature intervals of pearlite formation.
Název v anglickém jazyce
Study of kinetics phase transformations after plastic deformation of rail steel class IH alloyed with chromium
Popis výsledku anglicky
The paper is aimed at evaluation of effect previous plastic deformation on transformation kinetics of rail steel class IH alloyed with chromium. The CCT and DCCT diagrams were assembled on the basis of dilatometric tests with and/or without an influence of the previous deformation. To the experiment execution the dilation module of the plastometer Gleeble 3800 was used. The Accuracy of the diagrams was faced with metallographic analysis and measurement of hardness. The obtained results were compared with the results of in-process measurement of rail rolling mill Třinecké železárny Inc. This confirmed the theory that in the case of steels which are intended for rolling rails, no influence of the previous deformation the crucial influence pearlitic transformation in terms of time, but in the case of higher cooling rate has deformation an appreciable effect on shift temperature intervals of pearlite formation.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JG - Hutnictví, kovové materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/LO1203" target="_blank" >LO1203: Regionální materiálově technologické výzkumné centrum - Program udržitelnosti</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2016
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
METAL 2016 - 25th Anniversary International Conference on Metallurgy and Materials, Conference Proceedings
ISBN
978-80-87294-67-3
ISSN
—
e-ISSN
—
Počet stran výsledku
6
Strana od-do
403-408
Název nakladatele
Tanger Ltd
Místo vydání
Ostrava
Místo konání akce
Brno
Datum konání akce
25. 5. 2016
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
000391251200063