Raman study of PANI thin film during long time period in dependence on storage conditions
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27360%2F17%3A86099152" target="_blank" >RIV/61989100:27360/17:86099152 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/61989100:27640/17:86099152 RIV/61989100:27740/17:86099152
Výsledek na webu
<a href="https://link.springer.com/article/10.1007/s11696-016-0078-3" target="_blank" >https://link.springer.com/article/10.1007/s11696-016-0078-3</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1007/s11696-016-0078-3" target="_blank" >10.1007/s11696-016-0078-3</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Raman study of PANI thin film during long time period in dependence on storage conditions
Popis výsledku v původním jazyce
Conducting polymer polyaniline which is nowadays in forefront of the interest was in our study prepared in a form of thin films from anilinium sulfate by its chemical oxidation using ammonium peroxydisulfate. During the oxidation process, the polyaniline was deposited on glass slides and immersed into reaction mixture. Two sets of polyaniline thin films were prepared with different oxidation times (10, 20, 30, and 40 min). The first set was kept dry in desiccator and the second one was freely exposed to air moisture. Raman spectroscopy, nondestructive technique which is very sensitive to changes in structure of polymers, was used for the characterization of the protonation state of prepared polyaniline thin films. It was found that storage conditions affect the protonation state which in case of samples kept in desiccator is maintained without significant changes for longer time. Raman spectroscopy also revealed the dependence of protonation state on the oxidation time and 10 min proved as not sufficient for the creation of the protonation form of polyaniline. © 2016 Institute of Chemistry, Slovak Academy of Sciences
Název v anglickém jazyce
Raman study of PANI thin film during long time period in dependence on storage conditions
Popis výsledku anglicky
Conducting polymer polyaniline which is nowadays in forefront of the interest was in our study prepared in a form of thin films from anilinium sulfate by its chemical oxidation using ammonium peroxydisulfate. During the oxidation process, the polyaniline was deposited on glass slides and immersed into reaction mixture. Two sets of polyaniline thin films were prepared with different oxidation times (10, 20, 30, and 40 min). The first set was kept dry in desiccator and the second one was freely exposed to air moisture. Raman spectroscopy, nondestructive technique which is very sensitive to changes in structure of polymers, was used for the characterization of the protonation state of prepared polyaniline thin films. It was found that storage conditions affect the protonation state which in case of samples kept in desiccator is maintained without significant changes for longer time. Raman spectroscopy also revealed the dependence of protonation state on the oxidation time and 10 min proved as not sufficient for the creation of the protonation form of polyaniline. © 2016 Institute of Chemistry, Slovak Academy of Sciences
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
21001 - Nano-materials (production and properties)
Návaznosti výsledku
Projekt
<a href="/cs/project/LQ1602" target="_blank" >LQ1602: IT4Innovations excellence in science</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2017
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Chemical Papers
ISSN
0366-6352
e-ISSN
—
Svazek periodika
71
Číslo periodika v rámci svazku
2
Stát vydavatele periodika
CH - Švýcarská konfederace
Počet stran výsledku
7
Strana od-do
379-385
Kód UT WoS článku
000394523000015
EID výsledku v databázi Scopus
2-s2.0-85003828462