Study of heat capacities of Fe-C-Cr based metallic systems with use of DSC method and theoretical calculations
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27360%2F18%3A10241464" target="_blank" >RIV/61989100:27360/18:10241464 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Study of heat capacities of Fe-C-Cr based metallic systems with use of DSC method and theoretical calculations
Popis výsledku v původním jazyce
Seven alloys based on Fe-C-Cr were studied. Five alloys were model alloys based on Fe-C-Cr and there were compared with two steel with the similar composition. Model alloys contained carbon of 0.34 wt. % and chromium in a range of 0.92 - 4.76 wt. %. Steels contained carbon in the range 0.41 - 0.43 wt. % and chromium in the range 1.08 - 4.98 wt. %. Heat capacities were studied in a low and high-temperature region. The experimental heat capacities ("apparent heat capacities") were obtained using Differential Scanning Calorimetry (DSC) with use of a continuous method. The Setaram MHTC (Multi High-Temperature Calorimeter) 96 Line with a 3D DSC sensor was used for experiments with the use of DSC method. Measurements were done in an inert atmosphere of pure argon by a heating rate of 5oC/min. The experimental data were compared and discussed with the calculation results using SW Thermo Calc with the use of the TCFE8.1 (Thermo-Calc Fe-based alloys) database. Experimentally and theoretically obtained values for all alloys showed the same trend in the temperature range 474.15 - 950.15 K, 1188.15 - 1650.15 K and 1794.15 - 1853.15 K. The experimentally obtained heat capacities were within the range of 0.41 - 1.04 J/K.g. Steel with the content of carbon 0.41 wt. % and chromium 1.08 wt. % had values of heat capacities very close to model alloys in the low and high temperature area. Steel with the content of carbon 0.43 wt. % and chromium 4.98 wt. % had values of heat capacities higher than model alloys except for phase transformations.
Název v anglickém jazyce
Study of heat capacities of Fe-C-Cr based metallic systems with use of DSC method and theoretical calculations
Popis výsledku anglicky
Seven alloys based on Fe-C-Cr were studied. Five alloys were model alloys based on Fe-C-Cr and there were compared with two steel with the similar composition. Model alloys contained carbon of 0.34 wt. % and chromium in a range of 0.92 - 4.76 wt. %. Steels contained carbon in the range 0.41 - 0.43 wt. % and chromium in the range 1.08 - 4.98 wt. %. Heat capacities were studied in a low and high-temperature region. The experimental heat capacities ("apparent heat capacities") were obtained using Differential Scanning Calorimetry (DSC) with use of a continuous method. The Setaram MHTC (Multi High-Temperature Calorimeter) 96 Line with a 3D DSC sensor was used for experiments with the use of DSC method. Measurements were done in an inert atmosphere of pure argon by a heating rate of 5oC/min. The experimental data were compared and discussed with the calculation results using SW Thermo Calc with the use of the TCFE8.1 (Thermo-Calc Fe-based alloys) database. Experimentally and theoretically obtained values for all alloys showed the same trend in the temperature range 474.15 - 950.15 K, 1188.15 - 1650.15 K and 1794.15 - 1853.15 K. The experimentally obtained heat capacities were within the range of 0.41 - 1.04 J/K.g. Steel with the content of carbon 0.41 wt. % and chromium 1.08 wt. % had values of heat capacities very close to model alloys in the low and high temperature area. Steel with the content of carbon 0.43 wt. % and chromium 4.98 wt. % had values of heat capacities higher than model alloys except for phase transformations.
Klasifikace
Druh
O - Ostatní výsledky
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2018
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů