Concept of Damage Monitoring after Grinding for Components of Variable Hardness
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27640%2F16%3A86098471" target="_blank" >RIV/61989100:27640/16:86098471 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.mspro.2016.03.011" target="_blank" >http://dx.doi.org/10.1016/j.mspro.2016.03.011</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.mspro.2016.03.011" target="_blank" >10.1016/j.mspro.2016.03.011</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Concept of Damage Monitoring after Grinding for Components of Variable Hardness
Popis výsledku v původním jazyce
This paper deals with nondestructive magnetic evaluation of ground surfaces of chosen material hardness. The properties of prepared surfaces are studied with respect to the progressively worn grinding wheel. The nondestructive testing is based on the Barkhausen noise (BN) technique and obtained BN signals are supplemented by metallographic observations. The results show that the nature of thermal injury of the surfaces prepared by strongly worn grinding wheel significantly depends on the hardness of material. The typical thermal softening induced by grinding cycle is found on the surfaces of hardness 62 HRC whereas samples of lower hardness exhibit rehardening effect associated with the formation of white layer. These material changes are strongly correlated with the BN properties.
Název v anglickém jazyce
Concept of Damage Monitoring after Grinding for Components of Variable Hardness
Popis výsledku anglicky
This paper deals with nondestructive magnetic evaluation of ground surfaces of chosen material hardness. The properties of prepared surfaces are studied with respect to the progressively worn grinding wheel. The nondestructive testing is based on the Barkhausen noise (BN) technique and obtained BN signals are supplemented by metallographic observations. The results show that the nature of thermal injury of the surfaces prepared by strongly worn grinding wheel significantly depends on the hardness of material. The typical thermal softening induced by grinding cycle is found on the surfaces of hardness 62 HRC whereas samples of lower hardness exhibit rehardening effect associated with the formation of white layer. These material changes are strongly correlated with the BN properties.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
BM - Fyzika pevných látek a magnetismus
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/ED1.1.00%2F02.0070" target="_blank" >ED1.1.00/02.0070: Centrum excelence IT4Innovations</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2016
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Procedia Materials Science. Volume 12
ISBN
—
ISSN
2211-8128
e-ISSN
—
Počet stran výsledku
6
Strana od-do
60-65
Název nakladatele
Elsevier
Místo vydání
Amsterdam
Místo konání akce
Ostrava
Datum konání akce
8. 9. 2014
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
000386622900011