FRACTURE SURFACE DIGITIZING OF SPECIMEN FROM DROP-WEIGHT TEAR TEST
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989100%3A27690%2F09%3A00022450" target="_blank" >RIV/61989100:27690/09:00022450 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
FRACTURE SURFACE DIGITIZING OF SPECIMEN FROM DROP-WEIGHT TEAR TEST
Popis výsledku v původním jazyce
There is always a need to determine a fraction of the ductile,and respectively, brittle fracture on the fracture surface of specimen examined using a drop-weight tear test (DWTT).Determination of the percentage of ductile fracture (PDF) in accordance with valid national and international recommendations is not entirely unambiguousResults of evaluation show a large scattering for each criterion, and depend on the subjective view of the evaluator. Criteria are complex in nature and are independent of thefracture morphology. The dimensionless areas ratio criterion has been newly proposed for the evaluation of the DWTT specimens.This criterion is given by the ratio of the fracture surface projection into a base plane to the scanned fracture surface.The fracture surface of the DWTT specimen is scanned using a 3D-Cam scanner into a network of discrete points.A fracture surface area is calculated from the sum of the areas of triangles constructed above the element of the projection of fractu
Název v anglickém jazyce
FRACTURE SURFACE DIGITIZING OF SPECIMEN FROM DROP-WEIGHT TEAR TEST
Popis výsledku anglicky
There is always a need to determine a fraction of the ductile,and respectively, brittle fracture on the fracture surface of specimen examined using a drop-weight tear test (DWTT).Determination of the percentage of ductile fracture (PDF) in accordance with valid national and international recommendations is not entirely unambiguousResults of evaluation show a large scattering for each criterion, and depend on the subjective view of the evaluator. Criteria are complex in nature and are independent of thefracture morphology. The dimensionless areas ratio criterion has been newly proposed for the evaluation of the DWTT specimens.This criterion is given by the ratio of the fracture surface projection into a base plane to the scanned fracture surface.The fracture surface of the DWTT specimen is scanned using a 3D-Cam scanner into a network of discrete points.A fracture surface area is calculated from the sum of the areas of triangles constructed above the element of the projection of fractu
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JR - Ostatní strojírenství
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2009
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Sborník vědeckých prací VŠB -Technické univerzity Ostrava. Řada strojní
ISSN
1210-0471
e-ISSN
—
Svazek periodika
LV
Číslo periodika v rámci svazku
3
Stát vydavatele periodika
CZ - Česká republika
Počet stran výsledku
8
Strana od-do
—
Kód UT WoS článku
—
EID výsledku v databázi Scopus
—