Depth-Selective Study of Surface Crystallization in NANOPERM-Type Alloys
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F61989592%3A15310%2F14%3A33151747" target="_blank" >RIV/61989592:15310/14:33151747 - isvavai.cz</a>
Výsledek na webu
<a href="http://przyrbwn.icm.edu.pl/APP/PDF/126/a126z1p024.pdf" target="_blank" >http://przyrbwn.icm.edu.pl/APP/PDF/126/a126z1p024.pdf</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.12693/APhysPolA.126.56" target="_blank" >10.12693/APhysPolA.126.56</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Depth-Selective Study of Surface Crystallization in NANOPERM-Type Alloys
Popis výsledku v původním jazyce
Evolution of structure and magnetic order is studied in the 57Fe81Mo8Cu1B10 alloy by conversion electron and conversion X-ray 57Fe Mössbauer spectrometry. Surface features exhibit dierences at both sides of ribbon-shaped samples with respect to the screening depth. In the as-quenched state, traces of magnetite (in addition to bcc-Fe) are revealed only at the wheel side of the ribbon to the depth of about 200 nm. It is present also after annealing up to 510 C, then it disappears. In deeper regions (downto 1 m), magnetite is less abundant. At the air side, onlybcc-Fe is detected, though the progress of crystallization is more pronounced here than at the wheel side. Vibration properties of the bulk of amorphous and nanocrystalline samples are obtained from experiments of nuclear inelasticscattering of synchrotron radiation using partial densities of phonon states.
Název v anglickém jazyce
Depth-Selective Study of Surface Crystallization in NANOPERM-Type Alloys
Popis výsledku anglicky
Evolution of structure and magnetic order is studied in the 57Fe81Mo8Cu1B10 alloy by conversion electron and conversion X-ray 57Fe Mössbauer spectrometry. Surface features exhibit dierences at both sides of ribbon-shaped samples with respect to the screening depth. In the as-quenched state, traces of magnetite (in addition to bcc-Fe) are revealed only at the wheel side of the ribbon to the depth of about 200 nm. It is present also after annealing up to 510 C, then it disappears. In deeper regions (downto 1 m), magnetite is less abundant. At the air side, onlybcc-Fe is detected, though the progress of crystallization is more pronounced here than at the wheel side. Vibration properties of the bulk of amorphous and nanocrystalline samples are obtained from experiments of nuclear inelasticscattering of synchrotron radiation using partial densities of phonon states.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
BM - Fyzika pevných látek a magnetismus
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2014
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Acta Physica Polonica A
ISSN
0587-4246
e-ISSN
—
Svazek periodika
126
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
PL - Polská republika
Počet stran výsledku
2
Strana od-do
56-57
Kód UT WoS článku
000339833100025
EID výsledku v databázi Scopus
—