The effect of heat and ammonia treatment on colour response of oak wood (Quercus robur L.) and comparison of some physical and mechanical properties
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F62156489%3A43410%2F13%3A00208748" target="_blank" >RIV/62156489:43410/13:00208748 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
The effect of heat and ammonia treatment on colour response of oak wood (Quercus robur L.) and comparison of some physical and mechanical properties
Popis výsledku v původním jazyce
In this paper the effect of heat and ammonia treatment on the change in colour of oak wood (Quercus robur.) and comparison of physical and mechanical properties were investigated. Wood specimens were made from heartwood and sapwood in dimensions 30x30x30mm3. The specimens were subjected to heat treatment at 180°C and 230°C for 2 and 4 hours, others were treated by ammonia for 24 hours. After these processes, CIELAB colour, hardness, EMC, density and MOE of wood were tested in comparison with untreatedsamples. The results show that the heat treatment contributed to darkening of sapwood and heartwood and the total colour change increased up to 38.47 units (CIELAB) in the radial direction and 37.75 units (CIELAB) in the tangential direction. Previous research into ammonia treatment shows that the most significant changes were noticed after 1 day. The colour changes between sapwood and heartwood were more noticeable in ammonia treatment than in the case of heat treatment. All other obser
Název v anglickém jazyce
The effect of heat and ammonia treatment on colour response of oak wood (Quercus robur L.) and comparison of some physical and mechanical properties
Popis výsledku anglicky
In this paper the effect of heat and ammonia treatment on the change in colour of oak wood (Quercus robur.) and comparison of physical and mechanical properties were investigated. Wood specimens were made from heartwood and sapwood in dimensions 30x30x30mm3. The specimens were subjected to heat treatment at 180°C and 230°C for 2 and 4 hours, others were treated by ammonia for 24 hours. After these processes, CIELAB colour, hardness, EMC, density and MOE of wood were tested in comparison with untreatedsamples. The results show that the heat treatment contributed to darkening of sapwood and heartwood and the total colour change increased up to 38.47 units (CIELAB) in the radial direction and 37.75 units (CIELAB) in the tangential direction. Previous research into ammonia treatment shows that the most significant changes were noticed after 1 day. The colour changes between sapwood and heartwood were more noticeable in ammonia treatment than in the case of heat treatment. All other obser
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JJ - Ostatní materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/EE2.3.20.0269" target="_blank" >EE2.3.20.0269: Vytvoření mezinárodního vědecko-výzkumného týmu pro vývoj nových materiálů na bázi dřeva</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2013
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Maderas. Ciencia y tecnología
ISSN
0718-221X
e-ISSN
—
Svazek periodika
15
Číslo periodika v rámci svazku
3
Stát vydavatele periodika
CL - Chilská republika
Počet stran výsledku
15
Strana od-do
375-389
Kód UT WoS článku
326385400010
EID výsledku v databázi Scopus
—