Densification of beech wood and fixation of compressive deformation by steaming at lower temperatures
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F62156489%3A43410%2F16%3A00091948" target="_blank" >RIV/62156489:43410/16:00091948 - isvavai.cz</a>
Výsledek na webu
<a href="http://publicatio.nyme.hu/1056/1/Hardwood_2016_Proceedings_final_cover.pdf" target="_blank" >http://publicatio.nyme.hu/1056/1/Hardwood_2016_Proceedings_final_cover.pdf</a>
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Densification of beech wood and fixation of compressive deformation by steaming at lower temperatures
Popis výsledku v původním jazyce
The process of wood plasticization and densification that improves mechanical properties has been known for decades, but the utilization in wet conditions is limited due to the problems with dimensional stability. The deformation produced during the process is not stable and recovers almost totally when re-moistened and heated. This phenomenon is known as compression set recovery (KUTNAR, KAMKE 2012) or shape memory (NAVI, SANDBERG 2012). Treatment in high temperatures can decrease the compression set recovery, but mechanical properties are negatively affected (HILL 2006). Process with saturated steam is more efficient (KUTNAR, KAMKE 2012), so that complete fixation can be reached for example in 20 min at 180oC or 4 min at 200oC (NAVI, SANDBERG 2012). The process with lower temperatures takes more time; however, the mechanical properties are less decreased (HEGER 2004).
Název v anglickém jazyce
Densification of beech wood and fixation of compressive deformation by steaming at lower temperatures
Popis výsledku anglicky
The process of wood plasticization and densification that improves mechanical properties has been known for decades, but the utilization in wet conditions is limited due to the problems with dimensional stability. The deformation produced during the process is not stable and recovers almost totally when re-moistened and heated. This phenomenon is known as compression set recovery (KUTNAR, KAMKE 2012) or shape memory (NAVI, SANDBERG 2012). Treatment in high temperatures can decrease the compression set recovery, but mechanical properties are negatively affected (HILL 2006). Process with saturated steam is more efficient (KUTNAR, KAMKE 2012), so that complete fixation can be reached for example in 20 min at 180oC or 4 min at 200oC (NAVI, SANDBERG 2012). The process with lower temperatures takes more time; however, the mechanical properties are less decreased (HEGER 2004).
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
—
OECD FORD obor
20502 - Paper and wood
Návaznosti výsledku
Projekt
—
Návaznosti
S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2016
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Proceedings of the Eco-efficient resource wood with special focus on hardwoods
ISBN
978-963-334-291-6
ISSN
—
e-ISSN
—
Počet stran výsledku
3
Strana od-do
42-44
Název nakladatele
University of West Hungary
Místo vydání
Sopron
Místo konání akce
Sopron
Datum konání akce
8. 9. 2016
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
000473720100016