Influence of pressing parameters on surface properties of compressed beech wood
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F62156489%3A43410%2F17%3A43912927" target="_blank" >RIV/62156489:43410/17:43912927 - isvavai.cz</a>
Výsledek na webu
<a href="http://www.woodresearch.sk/wr/201706/11.pdf" target="_blank" >http://www.woodresearch.sk/wr/201706/11.pdf</a>
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Influence of pressing parameters on surface properties of compressed beech wood
Popis výsledku v původním jazyce
The influence of press conditions on wood properties was studied on densified beech wood. The pressing parameters affected the surface properties of wood specimens: hardness, roughness, and colour change. The effects and impacts varied among the individual pressing parameters and among the individual wood properties. Hardness was considerably improved by compression. The 40 % compression increased the hardness of the specimens by 2.4 to 3.4 times that of the original wood. The compression also noticeably reduced the wood surface roughness and smoothed the differences in roughness between the parallel and perpendicular directions. A higher pressing temperature and longer pressing time also caused significant changes in the wood colour. Lightness decreased, with the a* coordinate shifting to red and the b* coordinate shifting to yellow. The analysis of the results showed that the most suitable conditions for beech wood compression were: initial moisture content of 17 to 20 %, pressing temperature of 180 to 200oC, and pressing time, corresponding to the thickness of specimens, at least 10 min. For density, hardness, and roughness, more favourable results were obtained under 40 % compression.
Název v anglickém jazyce
Influence of pressing parameters on surface properties of compressed beech wood
Popis výsledku anglicky
The influence of press conditions on wood properties was studied on densified beech wood. The pressing parameters affected the surface properties of wood specimens: hardness, roughness, and colour change. The effects and impacts varied among the individual pressing parameters and among the individual wood properties. Hardness was considerably improved by compression. The 40 % compression increased the hardness of the specimens by 2.4 to 3.4 times that of the original wood. The compression also noticeably reduced the wood surface roughness and smoothed the differences in roughness between the parallel and perpendicular directions. A higher pressing temperature and longer pressing time also caused significant changes in the wood colour. Lightness decreased, with the a* coordinate shifting to red and the b* coordinate shifting to yellow. The analysis of the results showed that the most suitable conditions for beech wood compression were: initial moisture content of 17 to 20 %, pressing temperature of 180 to 200oC, and pressing time, corresponding to the thickness of specimens, at least 10 min. For density, hardness, and roughness, more favourable results were obtained under 40 % compression.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20502 - Paper and wood
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2017
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Wood Research
ISSN
1336-4561
e-ISSN
—
Svazek periodika
62
Číslo periodika v rámci svazku
6
Stát vydavatele periodika
SK - Slovenská republika
Počet stran výsledku
12
Strana od-do
939-950
Kód UT WoS článku
000424275700011
EID výsledku v databázi Scopus
2-s2.0-85040632202