About the determination of the thermal and athermal stress
Popis výsledku v původním jazyce
The determination of the thermal and athermal stress components using relaxation experiments along a stress?strain curve is critically evaluated. Short-term stress-relaxations are performed along the stress?strain curve of single crystals of Ge at 850K,Cu, and Ni3Al at 300K. They are analyzed by three different equations with two or three parameters including the athermal stress. The stress components obtained are compared to the values determined by stress-reduction experiments considered as the reference method. The relaxation rate is considered successively to be a power function or a hyperbolic sine function of the effective stress or a hyperbolic decrease of stress with time is assumed. It is shown that the three methods overestimate or underestimate the stress components depending on the material and deformation conditions. The error can be as large as about 100%. Reasons for the inadequacy of short-term relaxation experiments for the determination of the stress components are d
Název v anglickém jazyce
About the determination of the thermal and athermal stress
Popis výsledku anglicky
The determination of the thermal and athermal stress components using relaxation experiments along a stress?strain curve is critically evaluated. Short-term stress-relaxations are performed along the stress?strain curve of single crystals of Ge at 850K,Cu, and Ni3Al at 300K. They are analyzed by three different equations with two or three parameters including the athermal stress. The stress components obtained are compared to the values determined by stress-reduction experiments considered as the reference method. The relaxation rate is considered successively to be a power function or a hyperbolic sine function of the effective stress or a hyperbolic decrease of stress with time is assumed. It is shown that the three methods overestimate or underestimate the stress components depending on the material and deformation conditions. The error can be as large as about 100%. Reasons for the inadequacy of short-term relaxation experiments for the determination of the stress components are d
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
BM - Fyzika pevných látek a magnetismus
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2008
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Acta Materialia
ISSN
1359-6454
e-ISSN
—
Svazek periodika
56
Číslo periodika v rámci svazku
3
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
8
Strana od-do
333-340
Kód UT WoS článku
—
EID výsledku v databázi Scopus
—