Influence of thermal treatment on structure and microhardness of Fe75Ni2Si8B13C2 amorphous alloy
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68081723%3A_____%2F11%3A00376444" target="_blank" >RIV/68081723:_____/11:00376444 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.intermet.2011.07.027" target="_blank" >http://dx.doi.org/10.1016/j.intermet.2011.07.027</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.intermet.2011.07.027" target="_blank" >10.1016/j.intermet.2011.07.027</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Influence of thermal treatment on structure and microhardness of Fe75Ni2Si8B13C2 amorphous alloy
Popis výsledku v původním jazyce
Correlation between hardness of amorphous Fe75Ni2Si8B13C2 alloy and thermally induced structural transformations has been investigated by measuring microhardness in a series of samples heated at different temperatures from 25 to 1000 °C. The alloy has arelatively high hardness in the amorphous state, due to its chemical composition involving silicon, boron and carbon. As the alloy begins to crystallize, microhardness increased and reached a plateau in 500-650 °C temperature region, due to formation composite structure involving the small nanocrystals of alpha-Fe(Si) and Fe2B phases dispersed in the amorphous matrix. After treatment at higher temperatures, the nanocomposite structure is replaced by a more granulated structure, leading to decline in microhardness.
Název v anglickém jazyce
Influence of thermal treatment on structure and microhardness of Fe75Ni2Si8B13C2 amorphous alloy
Popis výsledku anglicky
Correlation between hardness of amorphous Fe75Ni2Si8B13C2 alloy and thermally induced structural transformations has been investigated by measuring microhardness in a series of samples heated at different temperatures from 25 to 1000 °C. The alloy has arelatively high hardness in the amorphous state, due to its chemical composition involving silicon, boron and carbon. As the alloy begins to crystallize, microhardness increased and reached a plateau in 500-650 °C temperature region, due to formation composite structure involving the small nanocrystals of alpha-Fe(Si) and Fe2B phases dispersed in the amorphous matrix. After treatment at higher temperatures, the nanocomposite structure is replaced by a more granulated structure, leading to decline in microhardness.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
BM - Fyzika pevných látek a magnetismus
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/1M0512" target="_blank" >1M0512: Centrrum výzkumu práškových nanomateriálů</a><br>
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2011
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Intermetallics
ISSN
0966-9795
e-ISSN
—
Svazek periodika
19
Číslo periodika v rámci svazku
7
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
6
Strana od-do
1780-1785