Strategies to Optimize the Strength and Fracture Resistance of Ceramic Laminates
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68081723%3A_____%2F12%3A00385918" target="_blank" >RIV/68081723:_____/12:00385918 - isvavai.cz</a>
Výsledek na webu
<a href="http://onlinelibrary.wiley.com/doi/10.1002/9781118217467.ch16/summary" target="_blank" >http://onlinelibrary.wiley.com/doi/10.1002/9781118217467.ch16/summary</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1002/9781118217467.ch16" target="_blank" >10.1002/9781118217467.ch16</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Strategies to Optimize the Strength and Fracture Resistance of Ceramic Laminates
Popis výsledku v původním jazyce
Layered ceramics, compared to conventional monolithic ceramics, are good choices for highly- loaded structural applications because they exhibit greater fracture resistance, higher strengths and better mechanical reliability (i.e. they are flaw tolerantmaterials). The use of tailored residual compressive stresses in the layers is a key parameter to adjust these properties. In this work ceramic laminates are analyzed which have internal residual compressive stresses. The most important factors having influence on the strength and fracture resistance of these laminates are discussed. A fracture mechanics analysis is employed to estimate the crack growth resistance of the material as a function of the crack length. It is found that the proper selection of a suitable strain mismatch (responsible for the generation of residual stresses), volume ratio of the layer materials and thickness and distribution of individual layers are crucial to achieve a high fracture resistance and/or a high lo
Název v anglickém jazyce
Strategies to Optimize the Strength and Fracture Resistance of Ceramic Laminates
Popis výsledku anglicky
Layered ceramics, compared to conventional monolithic ceramics, are good choices for highly- loaded structural applications because they exhibit greater fracture resistance, higher strengths and better mechanical reliability (i.e. they are flaw tolerantmaterials). The use of tailored residual compressive stresses in the layers is a key parameter to adjust these properties. In this work ceramic laminates are analyzed which have internal residual compressive stresses. The most important factors having influence on the strength and fracture resistance of these laminates are discussed. A fracture mechanics analysis is employed to estimate the crack growth resistance of the material as a function of the crack length. It is found that the proper selection of a suitable strain mismatch (responsible for the generation of residual stresses), volume ratio of the layer materials and thickness and distribution of individual layers are crucial to achieve a high fracture resistance and/or a high lo
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JH - Keramika, žáruvzdorné materiály a skla
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2012
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Mechanical Properties and Performance of Engineering Ceramics and Composites VII
ISBN
9781118205884
ISSN
—
e-ISSN
—
Počet stran výsledku
12
Strana od-do
163-174
Název nakladatele
John Wiley & Sons, Inc.,
Místo vydání
Hoboken, NJ, USA
Místo konání akce
Daytona Beach, Florida
Datum konání akce
24. 1. 2012
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—