Microstructural changes of AISI 316L due to structural sensitization and its influence on the fatigue properties
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68081723%3A_____%2F14%3A00436660" target="_blank" >RIV/68081723:_____/14:00436660 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Microstructural changes of AISI 316L due to structural sensitization and its influence on the fatigue properties
Popis výsledku v původním jazyce
Mechanical and fatigue properties of material are dependent on its microstructure. The microstructure of AISI 316L stainless steel commonly used for the production of medical tools, equipment and implants and during the operation they can be exposed to elevated temperatures. Microstructural changes and fatigue properties of AISI 316L stainless steel due to the heat treatment consisted of annealing at the temperature of 815°C with the dwell time of 500 hours were analyzed in the present paper. Precipitation of intermetallic phases and carbides was observed as a response of the material to the applied heat treatment. Negative influence was on the fatigue strength was observed in the case of region bellow N = 105 cycles; however the fatigue limit remainsunchanged despite to the structural sensitization.
Název v anglickém jazyce
Microstructural changes of AISI 316L due to structural sensitization and its influence on the fatigue properties
Popis výsledku anglicky
Mechanical and fatigue properties of material are dependent on its microstructure. The microstructure of AISI 316L stainless steel commonly used for the production of medical tools, equipment and implants and during the operation they can be exposed to elevated temperatures. Microstructural changes and fatigue properties of AISI 316L stainless steel due to the heat treatment consisted of annealing at the temperature of 815°C with the dwell time of 500 hours were analyzed in the present paper. Precipitation of intermetallic phases and carbides was observed as a response of the material to the applied heat treatment. Negative influence was on the fatigue strength was observed in the case of region bellow N = 105 cycles; however the fatigue limit remainsunchanged despite to the structural sensitization.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JL - Únava materiálu a lomová mechanika
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2014
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Materiálové inžinierstvo - Materials Engineering
ISSN
1335-0803
e-ISSN
—
Svazek periodika
21
Číslo periodika v rámci svazku
4
Stát vydavatele periodika
SK - Slovenská republika
Počet stran výsledku
6
Strana od-do
172-177
Kód UT WoS článku
—
EID výsledku v databázi Scopus
—