Crystal growth and characterisation of (DyxLa1-x)(2)Ti2O7 crystals
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68081723%3A_____%2F20%3A00533862" target="_blank" >RIV/68081723:_____/20:00533862 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/00216305:26620/20:PU139264
Výsledek na webu
<a href="http://www.elis.sk/index.php?page=shop.product_details&flypage=flypage.tpl&product_id=6595&category_id=162&option=com_virtuemart&vmcchk=1&Itemid=1" target="_blank" >http://www.elis.sk/index.php?page=shop.product_details&flypage=flypage.tpl&product_id=6595&category_id=162&option=com_virtuemart&vmcchk=1&Itemid=1</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.4149/km_2020_1_59" target="_blank" >10.4149/km_2020_1_59</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Crystal growth and characterisation of (DyxLa1-x)(2)Ti2O7 crystals
Popis výsledku v původním jazyce
LaTiO3.5 crystals were grown by optical floating zone technique in air, O-2, or Ar. Crystal structure varies between orthorhombic Pna2(1) (air, O-2) and monoclinic P2(1) (Ar). Crystals are transparent (air, O-2) or opaque (Ar) with amber or black colour. Magnetisation resembles the properties of LaTiO3.5. (DyxLa1-x)(2)Ti2O7 crystals were grown in O-2. The solubility of dopant (La or Dy) in the parent compound is limited. Two phases with Pna2(1) and Fd (3) over barm structure coexist in the range from x = 0.32 to 0.68. The a-axis of Pna2(1) is intact by substitution of La3+ by Dy3+, both b - and c-axes decrease. The a-axis of Fd (3) over barm increases with substitution of Dy3+ by La3+ and the spin freezing temperature T-f shifts to a higher temperature. Either of the new magnetic phase (Pna2(1) structure) or dynamical behaviour of spins in Fd (3) over barm phase exists below x = 0.68 in the range between the transition to 'spin ice' state T-i and T-f.
Název v anglickém jazyce
Crystal growth and characterisation of (DyxLa1-x)(2)Ti2O7 crystals
Popis výsledku anglicky
LaTiO3.5 crystals were grown by optical floating zone technique in air, O-2, or Ar. Crystal structure varies between orthorhombic Pna2(1) (air, O-2) and monoclinic P2(1) (Ar). Crystals are transparent (air, O-2) or opaque (Ar) with amber or black colour. Magnetisation resembles the properties of LaTiO3.5. (DyxLa1-x)(2)Ti2O7 crystals were grown in O-2. The solubility of dopant (La or Dy) in the parent compound is limited. Two phases with Pna2(1) and Fd (3) over barm structure coexist in the range from x = 0.32 to 0.68. The a-axis of Pna2(1) is intact by substitution of La3+ by Dy3+, both b - and c-axes decrease. The a-axis of Fd (3) over barm increases with substitution of Dy3+ by La3+ and the spin freezing temperature T-f shifts to a higher temperature. Either of the new magnetic phase (Pna2(1) structure) or dynamical behaviour of spins in Fd (3) over barm phase exists below x = 0.68 in the range between the transition to 'spin ice' state T-i and T-f.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2020
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Kovové materiály
ISSN
0023-432X
e-ISSN
—
Svazek periodika
58
Číslo periodika v rámci svazku
1
Stát vydavatele periodika
SK - Slovenská republika
Počet stran výsledku
12
Strana od-do
59-70
Kód UT WoS článku
000514823200007
EID výsledku v databázi Scopus
2-s2.0-85084242634