Determination of fatigue crack growth in the near-threshold regime using small-scale specimens
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68081723%3A_____%2F22%3A00557098" target="_blank" >RIV/68081723:_____/22:00557098 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/00216305:26110/22:PU144052
Výsledek na webu
<a href="https://www.sciencedirect.com/science/article/pii/S0167844221003207?via%3Dihub" target="_blank" >https://www.sciencedirect.com/science/article/pii/S0167844221003207?via%3Dihub</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.tafmec.2021.103224" target="_blank" >10.1016/j.tafmec.2021.103224</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Determination of fatigue crack growth in the near-threshold regime using small-scale specimens
Popis výsledku v původním jazyce
A complete description of the experimental procedure for characterizing the intrinsic fatigue crack propagation threshold (delta(Kth,eff)) as well as the fatigue crack growth rate (FCGR) in the near-threshold regime using small-scale specimens is presented. A comparative study is carried out on the high strength steel S960QL considering different single edge notch bend (SENB) specimen geometries. On one hand, the reference dimensions of 6 mm thickness (B) and 19 mm width (W) are analysed and referred to as conventional specimens. On the other hand, small-scale specimens with B = 3 mm and W = 4 and 6 mm are also considered. Several loading configurations (3, 4-and 8-point bending) are used and a load ratio R = 0.8 is applied to avoid crack closure effects. The direct current potential drop (DCPD) technique is used to monitor the crack length. The reduced dimensions of the small-scale specimens imply the necessity of implementing a modified testing procedure compared to the recommendations of current standards for the generation of FCGR data. The results show a good agreement between tests conducted on different specimen sizes, which opens new perspectives in the use of small-scale specimens for characterizing the fatigue crack growth properties in metallic materials. Recommendations and limitations of the procedure are provided and discussed.
Název v anglickém jazyce
Determination of fatigue crack growth in the near-threshold regime using small-scale specimens
Popis výsledku anglicky
A complete description of the experimental procedure for characterizing the intrinsic fatigue crack propagation threshold (delta(Kth,eff)) as well as the fatigue crack growth rate (FCGR) in the near-threshold regime using small-scale specimens is presented. A comparative study is carried out on the high strength steel S960QL considering different single edge notch bend (SENB) specimen geometries. On one hand, the reference dimensions of 6 mm thickness (B) and 19 mm width (W) are analysed and referred to as conventional specimens. On the other hand, small-scale specimens with B = 3 mm and W = 4 and 6 mm are also considered. Several loading configurations (3, 4-and 8-point bending) are used and a load ratio R = 0.8 is applied to avoid crack closure effects. The direct current potential drop (DCPD) technique is used to monitor the crack length. The reduced dimensions of the small-scale specimens imply the necessity of implementing a modified testing procedure compared to the recommendations of current standards for the generation of FCGR data. The results show a good agreement between tests conducted on different specimen sizes, which opens new perspectives in the use of small-scale specimens for characterizing the fatigue crack growth properties in metallic materials. Recommendations and limitations of the procedure are provided and discussed.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20102 - Construction engineering, Municipal and structural engineering
Návaznosti výsledku
Projekt
<a href="/cs/project/GA20-00761S" target="_blank" >GA20-00761S: Vliv materiálových vlastností korozivzdorných ocelí na spolehlivost mostních konstrukcí</a><br>
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2022
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Theoretical and Applied Fracture Mechanics
ISSN
0167-8442
e-ISSN
1872-7638
Svazek periodika
118
Číslo periodika v rámci svazku
APR
Stát vydavatele periodika
NL - Nizozemsko
Počet stran výsledku
12
Strana od-do
103224
Kód UT WoS článku
000781771300004
EID výsledku v databázi Scopus
2-s2.0-85122229577