CsI:Tl+,Yb2+: ultra-high light yield scintillator with reduced afterglow
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68378271%3A_____%2F14%3A00432572" target="_blank" >RIV/68378271:_____/14:00432572 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1039/c3ce42645a" target="_blank" >http://dx.doi.org/10.1039/c3ce42645a</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1039/c3ce42645a" target="_blank" >10.1039/c3ce42645a</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
CsI:Tl+,Yb2+: ultra-high light yield scintillator with reduced afterglow
Popis výsledku v původním jazyce
The afterglow problem has been preventing CsI:Tl single crystal scintillators from being used for applications in the field of computer tomography and high-speed imaging. We show that Yb2+ codoping in CsI:Tl can reduce it at least by one order of magnitude after 50 ms from X-ray cut-off compared to ordinary CsI:Tl. After optimization of the Yb2+ and Tl+ concentrations, the doubly doped CsI:Tl,Yb crystal exhibits an ultra-high light yield of 90 000 6000 photons MeV1, energy resolution 7.9%@511 keV and low afterglow level of about 0.035% at 80 ms. Simultaneous improvement in afterglow, light yield and energy resolution in CsI:Tl-based scintillators paves the way to its application in computer tomography and high-speed imaging. The physical mechanism androle of ytterbium ions in afterglow suppression are proposed.
Název v anglickém jazyce
CsI:Tl+,Yb2+: ultra-high light yield scintillator with reduced afterglow
Popis výsledku anglicky
The afterglow problem has been preventing CsI:Tl single crystal scintillators from being used for applications in the field of computer tomography and high-speed imaging. We show that Yb2+ codoping in CsI:Tl can reduce it at least by one order of magnitude after 50 ms from X-ray cut-off compared to ordinary CsI:Tl. After optimization of the Yb2+ and Tl+ concentrations, the doubly doped CsI:Tl,Yb crystal exhibits an ultra-high light yield of 90 000 6000 photons MeV1, energy resolution 7.9%@511 keV and low afterglow level of about 0.035% at 80 ms. Simultaneous improvement in afterglow, light yield and energy resolution in CsI:Tl-based scintillators paves the way to its application in computer tomography and high-speed imaging. The physical mechanism androle of ytterbium ions in afterglow suppression are proposed.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
BM - Fyzika pevných látek a magnetismus
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/LH12185" target="_blank" >LH12185: Inovativní scintilátory na bázi keramik, sklo-keramik a monokrystalů: uzpůsobení materiálu a fyzikální jevy</a><br>
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2014
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
CrystEngComm
ISSN
1466-8033
e-ISSN
—
Svazek periodika
16
Číslo periodika v rámci svazku
16
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
6
Strana od-do
3312-3317