Nondestructive indication of fatigue damage and residual lifetime in ferromagnetic construction materials
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68378271%3A_____%2F14%3A00432643" target="_blank" >RIV/68378271:_____/14:00432643 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/68407700:21340/14:00220475
Výsledek na webu
<a href="http://dx.doi.org/10.1088/0957-0233/25/6/065601" target="_blank" >http://dx.doi.org/10.1088/0957-0233/25/6/065601</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1088/0957-0233/25/6/065601" target="_blank" >10.1088/0957-0233/25/6/065601</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Nondestructive indication of fatigue damage and residual lifetime in ferromagnetic construction materials
Popis výsledku v původním jazyce
A new revolutionary attitude toward investigation of fatigue damage in cyclically loaded steel samples is reported. The measurement is based on the method of magnetic adaptive testing, which?in contrast to traditional magnetic hysteresis investigations?picks up the relevant information from systematic measurement and evaluation of whole minor magnetic hysteresis loops and their derivatives. Satisfactory correlations between nondestructively measured magnetic descriptors and actual lifetime of the fatigued material were found. The presented method is able to serve as a powerful tool for indication of changes, which occur in the structure of the inspected objects during their industrial service lifetime, as long as they are manufactured from ferromagnetic materials.
Název v anglickém jazyce
Nondestructive indication of fatigue damage and residual lifetime in ferromagnetic construction materials
Popis výsledku anglicky
A new revolutionary attitude toward investigation of fatigue damage in cyclically loaded steel samples is reported. The measurement is based on the method of magnetic adaptive testing, which?in contrast to traditional magnetic hysteresis investigations?picks up the relevant information from systematic measurement and evaluation of whole minor magnetic hysteresis loops and their derivatives. Satisfactory correlations between nondestructively measured magnetic descriptors and actual lifetime of the fatigued material were found. The presented method is able to serve as a powerful tool for indication of changes, which occur in the structure of the inspected objects during their industrial service lifetime, as long as they are manufactured from ferromagnetic materials.
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
BM - Fyzika pevných látek a magnetismus
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GAP108%2F12%2F1872" target="_blank" >GAP108/12/1872: Komplexní funkčně gradované materiály</a><br>
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2014
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Measurement Science and Technology
ISSN
0957-0233
e-ISSN
—
Svazek periodika
25
Číslo periodika v rámci svazku
6
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
10
Strana od-do
"065601-1"-"065601-10"
Kód UT WoS článku
000338562600046
EID výsledku v databázi Scopus
—