Highly luminescent cerium-doped YSO/ LSO microcrystals prepared via room temperature sol-gel route
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68378271%3A_____%2F19%3A00520333" target="_blank" >RIV/68378271:_____/19:00520333 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/68407700:21340/19:00328307
Výsledek na webu
<a href="https://doi.org/10.1016/j.radmeas.2019.01.012" target="_blank" >https://doi.org/10.1016/j.radmeas.2019.01.012</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.radmeas.2019.01.012" target="_blank" >10.1016/j.radmeas.2019.01.012</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Highly luminescent cerium-doped YSO/ LSO microcrystals prepared via room temperature sol-gel route
Popis výsledku v původním jazyce
Luminescent properties of Ce-doped yttrium oxyorthosilicate (Y2SiO5, YSO) and lutetium oxyorthosilicate (Lu2SiO5, LSO) prepared by a room-temperature sol-gel route were studied and compared to those of YSO and LSO single crystals. Structural changes in the samples during calcination were also studied by X-ray diffraction and differential thermal analysis. Radioluminescence spectra of the samples show comparable emission intensity with the bulk materials. Photoluminescence decay measurements were used to investigate the decay characteristics of the prepared powders. Changes in luminescent properties after the reduction of particle size by grinding in a ball mill were also demonstrated on the YSO:Ce3+ sample. Acceleration of the faster component of the decay time from 7.1 ns to 6.2 ns was observed. Prepared YSO:Ce3+ and LSO:Ce3+ powders are suggested to be good candidates for fast imaging or other applications.n
Název v anglickém jazyce
Highly luminescent cerium-doped YSO/ LSO microcrystals prepared via room temperature sol-gel route
Popis výsledku anglicky
Luminescent properties of Ce-doped yttrium oxyorthosilicate (Y2SiO5, YSO) and lutetium oxyorthosilicate (Lu2SiO5, LSO) prepared by a room-temperature sol-gel route were studied and compared to those of YSO and LSO single crystals. Structural changes in the samples during calcination were also studied by X-ray diffraction and differential thermal analysis. Radioluminescence spectra of the samples show comparable emission intensity with the bulk materials. Photoluminescence decay measurements were used to investigate the decay characteristics of the prepared powders. Changes in luminescent properties after the reduction of particle size by grinding in a ball mill were also demonstrated on the YSO:Ce3+ sample. Acceleration of the faster component of the decay time from 7.1 ns to 6.2 ns was observed. Prepared YSO:Ce3+ and LSO:Ce3+ powders are suggested to be good candidates for fast imaging or other applications.n
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
10403 - Physical chemistry
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2019
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Radiation Measurements
ISSN
1350-4487
e-ISSN
—
Svazek periodika
122
Číslo periodika v rámci svazku
Mar
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
7
Strana od-do
84-90
Kód UT WoS článku
000462798400015
EID výsledku v databázi Scopus
2-s2.0-85061272321