Use of a zirconium alloy coated with an homogeneous polycrystalline diamond layer for a nuclear reactor
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68378271%3A_____%2F20%3A00532446" target="_blank" >RIV/68378271:_____/20:00532446 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/68407700:21220/20:00347007 RIV/68407700:21730/20:00347007
Výsledek na webu
<a href="https://worldwide.espacenet.com/patent/search/family/051798943/publication/EP3047046A1?q=EP3047046" target="_blank" >https://worldwide.espacenet.com/patent/search/family/051798943/publication/EP3047046A1?q=EP3047046</a>
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Use of a zirconium alloy coated with an homogeneous polycrystalline diamond layer for a nuclear reactor
Popis výsledku v původním jazyce
A layer protecting the surface of zirconium alloys used as materials for nuclear reactors is formed by a homogenous polycrystalline diamond layer prepared by chemical vapor deposition method. This diamond layer is from 100 nm to 50 μm thick and the size of the crystalline cores in the layer ranges from 10 nm to 500 nm. Maximum content of non-diamond carbon is 25 mol%, total content of non-carbon impurities is maximum up to 0.5 mol%, RMS surface roughness of the polycrystalline diamond layer has a value less than 40 nm and thermal conductivity of the layer ranges from 1000 to 1900 W·m−1·K−1.nCoating of the zirconium alloys surface with the described polycrystalline diamond layer serves as a zirconium alloys surface protection against undesirable changes and processes in the nuclear reactor environment.nnPriorita CZ305059 - RIV: RIV/68378271:_____/15:00447999
Název v anglickém jazyce
Use of a zirconium alloy coated with an homogeneous polycrystalline diamond layer for a nuclear reactor
Popis výsledku anglicky
A layer protecting the surface of zirconium alloys used as materials for nuclear reactors is formed by a homogenous polycrystalline diamond layer prepared by chemical vapor deposition method. This diamond layer is from 100 nm to 50 μm thick and the size of the crystalline cores in the layer ranges from 10 nm to 500 nm. Maximum content of non-diamond carbon is 25 mol%, total content of non-carbon impurities is maximum up to 0.5 mol%, RMS surface roughness of the polycrystalline diamond layer has a value less than 40 nm and thermal conductivity of the layer ranges from 1000 to 1900 W·m−1·K−1.nCoating of the zirconium alloys surface with the described polycrystalline diamond layer serves as a zirconium alloys surface protection against undesirable changes and processes in the nuclear reactor environment.nnPriorita CZ305059 - RIV: RIV/68378271:_____/15:00447999
Klasifikace
Druh
P - Patent
CEP obor
—
OECD FORD obor
10304 - Nuclear physics
Návaznosti výsledku
Projekt
<a href="/cs/project/TA04020156" target="_blank" >TA04020156: Ochrana povrchu zirkoniových slitin kompozitními polykrystalickými diamantovými povlaky.</a><br>
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2020
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Číslo patentu nebo vzoru
EP3047046
Vydavatel
EPO_1 -
Název vydavatele
European Patent Office
Místo vydání
Munich, The Hague, Berlin, Vienna, Brussels
Stát vydání
—
Datum přijetí
19. 8. 2020
Název vlastníka
České vysoké učení technické v Praze, Fakuta strojní - Fyzikální ústav AV ČR, v. v. i
Způsob využití
A - Výsledek využívá pouze poskytovatel
Druh možnosti využití
A - K využití výsledku jiným subjektem je vždy nutné nabytí licence