Diamond coating reduces nuclear fuel rod corrosion at accidental temperatures: the role of surface electrochemistry and semiconductivity
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68378271%3A_____%2F21%3A00548786" target="_blank" >RIV/68378271:_____/21:00548786 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/60461373:22320/21:43922932 RIV/68407700:21340/21:00352443 RIV/68407700:21730/21:00352443
Výsledek na webu
<a href="http://hdl.handle.net/11104/0324956" target="_blank" >http://hdl.handle.net/11104/0324956</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.3390/ma14216315" target="_blank" >10.3390/ma14216315</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Diamond coating reduces nuclear fuel rod corrosion at accidental temperatures: the role of surface electrochemistry and semiconductivity
Popis výsledku v původním jazyce
To decrease probability of the accident in nuclear reactors, it is necessary to reduce the surface corrosion of Zr fuel rods. In this work we present the ability of diamond surface coating to protect ZIRLO nuclear fuel rod against corrosion under nuclear reactor accidental conditions. ZIRLO rod surface was coated by 500 nm diamond layer grown in a pulse microwave plasma chemical vapour deposition apparatus. We focused on the role of carbon phases and accidental temperatures (from 850oC to 1000 oC) in ZIRLO oxidation and hydrogen uptake processes. Dia-mond coating made strong barrier against hydrogen uptake into ZIRLO under all tested conditions.
Název v anglickém jazyce
Diamond coating reduces nuclear fuel rod corrosion at accidental temperatures: the role of surface electrochemistry and semiconductivity
Popis výsledku anglicky
To decrease probability of the accident in nuclear reactors, it is necessary to reduce the surface corrosion of Zr fuel rods. In this work we present the ability of diamond surface coating to protect ZIRLO nuclear fuel rod against corrosion under nuclear reactor accidental conditions. ZIRLO rod surface was coated by 500 nm diamond layer grown in a pulse microwave plasma chemical vapour deposition apparatus. We focused on the role of carbon phases and accidental temperatures (from 850oC to 1000 oC) in ZIRLO oxidation and hydrogen uptake processes. Dia-mond coating made strong barrier against hydrogen uptake into ZIRLO under all tested conditions.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20501 - Materials engineering
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2021
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Materials
ISSN
1996-1944
e-ISSN
1996-1944
Svazek periodika
14
Číslo periodika v rámci svazku
21
Stát vydavatele periodika
CH - Švýcarská konfederace
Počet stran výsledku
16
Strana od-do
6315
Kód UT WoS článku
000718436000001
EID výsledku v databázi Scopus
2-s2.0-85117852755