The effect of curvature of a pipe wall on the fracture toughness and protection of high pressure pipelines
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68378297%3A_____%2F16%3A00459000" target="_blank" >RIV/68378297:_____/16:00459000 - isvavai.cz</a>
Výsledek na webu
<a href="http://www.sciencedirect.com/science/article/pii/S2214785316002364" target="_blank" >http://www.sciencedirect.com/science/article/pii/S2214785316002364</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.matpr.2016.03.031" target="_blank" >10.1016/j.matpr.2016.03.031</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
The effect of curvature of a pipe wall on the fracture toughness and protection of high pressure pipelines
Popis výsledku v původním jazyce
For standard fracture mechanical tests flat specimens (principally CT or SENB) are required. When investigating fracture mechanical properties of thin – walled pipes this brings about a problem because it is necessary to straighten pipe bands. This operation causes internal stresses to be induced not only in the semi-product subjected to straightening but also in finished specimens. A question therefore arises to what extent are then the magnitudes of the fracture toughness determined representative for the actual cylindrical wall. To solve this problem fracture mechanics tests were carried out on flat (straightened) CT specimens as well as on curved CT specimens with the natural curvature. The R – curves as well as the resulting parameters of the fracture toughness, obtained for both types of CT specimens, were compared and it was concluded that the fracture toughness of the pipe material determined on straightened CT specimens was practically the same as that obtained on curved CT specimens.
Název v anglickém jazyce
The effect of curvature of a pipe wall on the fracture toughness and protection of high pressure pipelines
Popis výsledku anglicky
For standard fracture mechanical tests flat specimens (principally CT or SENB) are required. When investigating fracture mechanical properties of thin – walled pipes this brings about a problem because it is necessary to straighten pipe bands. This operation causes internal stresses to be induced not only in the semi-product subjected to straightening but also in finished specimens. A question therefore arises to what extent are then the magnitudes of the fracture toughness determined representative for the actual cylindrical wall. To solve this problem fracture mechanics tests were carried out on flat (straightened) CT specimens as well as on curved CT specimens with the natural curvature. The R – curves as well as the resulting parameters of the fracture toughness, obtained for both types of CT specimens, were compared and it was concluded that the fracture toughness of the pipe material determined on straightened CT specimens was practically the same as that obtained on curved CT specimens.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JL - Únava materiálu a lomová mechanika
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/TE02000162" target="_blank" >TE02000162: Centrum pokročilých materiálů a technologií pro ochranu a zvýšení bezpečnosti</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2016
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Materials Today: Proceedings
ISBN
—
ISSN
2214-7853
e-ISSN
—
Počet stran výsledku
6
Strana od-do
973-978
Název nakladatele
Elsevier
Místo vydání
Amsterdam
Místo konání akce
Starý Smokovec
Datum konání akce
22. 9. 2015
Typ akce podle státní příslušnosti
EUR - Evropská akce
Kód UT WoS článku
000373068900013