Influence of Casting Direction on Fracture Energy of Fiber-Reinforced Cement Composites
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68407700%3A21110%2F14%3A00210818" target="_blank" >RIV/68407700:21110/14:00210818 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.4028/www.scientific.net/KEM.594-595.444" target="_blank" >http://dx.doi.org/10.4028/www.scientific.net/KEM.594-595.444</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.4028/www.scientific.net/KEM.594-595.444" target="_blank" >10.4028/www.scientific.net/KEM.594-595.444</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Influence of Casting Direction on Fracture Energy of Fiber-Reinforced Cement Composites
Popis výsledku v původním jazyce
This paper is focused on behavior of fiber reinforced cement composites (FRC) and ultrahigh-performance fiber reinforced cement composites (UHPFRC) in dependence on the direction of casting. Twelve prismatic samples of size of 400 x 100 x 100 mm were cast into moulds; six of these were FRC and the other six were UHPFRC. Three samples of both series were cast in the common horizontal direction and the other three in the vertical way. It was found that fracture energy of horizontally cast prisms was approximately three times higher in both cases than the vertically cast ones. The peak loads of FRC were very similar for both ways of casting. On the other hand the UHPFRC behaved differently, the peak load of horizontally cast prisms was approximately 2,5 times higher than the vertically cast ones. It was demonstrated that these differences are caused by the way of casting and vibration.
Název v anglickém jazyce
Influence of Casting Direction on Fracture Energy of Fiber-Reinforced Cement Composites
Popis výsledku anglicky
This paper is focused on behavior of fiber reinforced cement composites (FRC) and ultrahigh-performance fiber reinforced cement composites (UHPFRC) in dependence on the direction of casting. Twelve prismatic samples of size of 400 x 100 x 100 mm were cast into moulds; six of these were FRC and the other six were UHPFRC. Three samples of both series were cast in the common horizontal direction and the other three in the vertical way. It was found that fracture energy of horizontally cast prisms was approximately three times higher in both cases than the vertically cast ones. The peak loads of FRC were very similar for both ways of casting. On the other hand the UHPFRC behaved differently, the peak load of horizontally cast prisms was approximately 2,5 times higher than the vertically cast ones. It was demonstrated that these differences are caused by the way of casting and vibration.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JN - Stavebnictví
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GAP104%2F12%2F0791" target="_blank" >GAP104/12/0791: Vláknové kompozity na bázi cementu pro vysokoteplotní aplikace</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2014
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Advanced Materials Engineering and Technology II
ISBN
978-3-03785-937-7
ISSN
1013-9826
e-ISSN
—
Počet stran výsledku
5
Strana od-do
444-448
Název nakladatele
Trans Tech Publications
Místo vydání
Uetikon-Zurich
Místo konání akce
Bandung
Datum konání akce
28. 11. 2013
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
000336337200080