Durability of structural adhesive joints for facade applications exposed to the extended cataplasm test
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68407700%3A21110%2F19%3A00329928" target="_blank" >RIV/68407700:21110/19:00329928 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/68407700:21610/19:00329928
Výsledek na webu
<a href="https://doi.org/10.1080/00218464.2019.1570157" target="_blank" >https://doi.org/10.1080/00218464.2019.1570157</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1080/00218464.2019.1570157" target="_blank" >10.1080/00218464.2019.1570157</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Durability of structural adhesive joints for facade applications exposed to the extended cataplasm test
Popis výsledku v původním jazyce
The effects of exposure to humid conditions in the extended cataplasm ageing test, based on ISO 9142, Procedure E2 on the mechanical properties of adhesively bonded joints, were investigated as a part of a comprehensive study on the ageing of an acrylate adhesive and a Silane-terminated polymer (STP) adhesive. The adhesives were applied in aluminium and Zn-electroplated steel substrates with various surface treatments (a smooth surface, a roughened surface, and anodized and blank aluminium) to observe the effect of ageing on joints with various substrates. The predominant effect of high relative humidity in the cataplasm test was compared with the results of immersion in water according to ETAG 002.
Název v anglickém jazyce
Durability of structural adhesive joints for facade applications exposed to the extended cataplasm test
Popis výsledku anglicky
The effects of exposure to humid conditions in the extended cataplasm ageing test, based on ISO 9142, Procedure E2 on the mechanical properties of adhesively bonded joints, were investigated as a part of a comprehensive study on the ageing of an acrylate adhesive and a Silane-terminated polymer (STP) adhesive. The adhesives were applied in aluminium and Zn-electroplated steel substrates with various surface treatments (a smooth surface, a roughened surface, and anodized and blank aluminium) to observe the effect of ageing on joints with various substrates. The predominant effect of high relative humidity in the cataplasm test was compared with the results of immersion in water according to ETAG 002.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20101 - Civil engineering
Návaznosti výsledku
Projekt
<a href="/cs/project/GA18-10907S" target="_blank" >GA18-10907S: Mechanické vlastnosti polymerních lepených spojů pro aplikace ve stavebnictví s ohledem na působení okolního prostředí a stárnutí</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2019
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
The Journal of Adhesion
ISSN
0021-8464
e-ISSN
1545-5823
Svazek periodika
95
Číslo periodika v rámci svazku
5-7
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
21
Strana od-do
632-652
Kód UT WoS článku
000471981600017
EID výsledku v databázi Scopus
2-s2.0-85066868560