Zjišťování zbytkových napětí u trubkových ohybů
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68407700%3A21220%2F03%3A02091593" target="_blank" >RIV/68407700:21220/03:02091593 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
čeština
Název v původním jazyce
Zjišťování zbytkových napětí u trubkových ohybů
Popis výsledku v původním jazyce
Residual stresses are induced in the material of structures in almost all manufacturing processes. Presence of residual stresses in construction is undesirable and plenty of finance is spent to remove or reduce it. Pipe bends are produced from rolled weldless pipe by hot forming under temperature between 920 - 980 °C and cooled from this temperature by means of air. Temper annealing is requared by SN standard 42 0284 in this case, because both ends of pipe were not warm. This operation is very expensiveand also has substantially increased production time and following production cost rise. New SN standard 130021-6-1 alows omit annealing operation in the case of the low level residual stresses in construction. Therefore residaul stresses were measuredin pipe bend. Hole drilling method was used for determination of residual stresses. Residual stresses were measured in 14 places on the surface of the pipe bend and in one place on comparing pipe. This article describes experiment sett.
Název v anglickém jazyce
Detection of Residual Stresses of the Pipe Bend
Popis výsledku anglicky
Residual stresses are induced in the material of structures in almost all manufacturing processes. Presence of residual stresses in construction is undesirable and plenty of finance is spent to remove or reduce it. Pipe bends are produced from rolled weldless pipe by hot forming under temperature between 920 - 980 °C and cooled from this temperature by means of air. Temper annealing is requared by SN standard 42 0284 in this case, because both ends of pipe were not warm. This operation is very expensiveand also has substantially increased production time and following production cost rise. New SN standard 130021-6-1 alows omit annealing operation in the case of the low level residual stresses in construction. Therefore residaul stresses were measuredin pipe bend. Hole drilling method was used for determination of residual stresses. Residual stresses were measured in 14 places on the surface of the pipe bend and in one place on comparing pipe. This article describes experiment sett.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JL - Únava materiálu a lomová mechanika
OECD FORD obor
—
Návaznosti výsledku
Projekt
Výsledek vznikl pri realizaci vícero projektů. Více informací v záložce Projekty.
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)
Ostatní
Rok uplatnění
2003
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Experimentální analýza napětí 2003
ISBN
80-214-2314-5
ISSN
—
e-ISSN
—
Počet stran výsledku
2
Strana od-do
15-16
Název nakladatele
VUT, Fakulta strojní
Místo vydání
Brno
Místo konání akce
Milovy
Datum konání akce
3. 6. 2003
Typ akce podle státní příslušnosti
CST - Celostátní akce
Kód UT WoS článku
—