Kinetics of Grain Growth and Recrystallization during Forming Modes for Processing of Steel SA 508
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68407700%3A21220%2F12%3A00193796" target="_blank" >RIV/68407700:21220/12:00193796 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Kinetics of Grain Growth and Recrystallization during Forming Modes for Processing of Steel SA 508
Popis výsledku v původním jazyce
Within the optimization of material processing technology for heavy forgings made from the steel SA 508 for power industry (especially shafts), kinetics of grain growth, recrystallization and precipitation processes in order to prevent the occurrence ofcoarse-grained structures were evaluated. In the typical range of forging temperatures of 850 °C - 1250 °C the austenite grain coarsens significantly above a temperature of 1100 °C. Evaluation of recrystallization processes shows significant inhibition of dynamic and consequently postdynamic recrystallization after deformation of 60 % at temperature 850 °C. With increasing deformation temperature the contribution of dynamic and postdynamic recrystallization grows. Particles present in the microstructureevaluated by TEM are mostly M3C type. The optimization of material processing technology forged steel SA 508 for power supply applications has been evaluated and grain growth kinetics of precipitation processes in order to prevent undesi
Název v anglickém jazyce
Kinetics of Grain Growth and Recrystallization during Forming Modes for Processing of Steel SA 508
Popis výsledku anglicky
Within the optimization of material processing technology for heavy forgings made from the steel SA 508 for power industry (especially shafts), kinetics of grain growth, recrystallization and precipitation processes in order to prevent the occurrence ofcoarse-grained structures were evaluated. In the typical range of forging temperatures of 850 °C - 1250 °C the austenite grain coarsens significantly above a temperature of 1100 °C. Evaluation of recrystallization processes shows significant inhibition of dynamic and consequently postdynamic recrystallization after deformation of 60 % at temperature 850 °C. With increasing deformation temperature the contribution of dynamic and postdynamic recrystallization grows. Particles present in the microstructureevaluated by TEM are mostly M3C type. The optimization of material processing technology forged steel SA 508 for power supply applications has been evaluated and grain growth kinetics of precipitation processes in order to prevent undesi
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JJ - Ostatní materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/FR-TI2%2F132" target="_blank" >FR-TI2/132: Výzkum příčin výrobních vad hmotných výkovků a odlitků s nejvyššími jakostními parametry pro parní, větrné a jaderné elektrárny</a><br>
Návaznosti
O - Projekt operacniho programu
Ostatní
Rok uplatnění
2012
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Metal 2012
ISBN
978-80-87294-29-1
ISSN
—
e-ISSN
—
Počet stran výsledku
6
Strana od-do
1-6
Název nakladatele
TANGER, spol.s r.o
Místo vydání
Ostrava
Místo konání akce
Brno
Datum konání akce
23. 5. 2012
Typ akce podle státní příslušnosti
EUR - Evropská akce
Kód UT WoS článku
—