Degradation the Refractories of Rotary Furnance Linnings in the Production of Zinc Oxide
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68407700%3A21220%2F13%3A00213204" target="_blank" >RIV/68407700:21220/13:00213204 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Degradation the Refractories of Rotary Furnance Linnings in the Production of Zinc Oxide
Popis výsledku v původním jazyce
This paper is closely connected with the complex problem of degradation relating to the refractories of rotary furnace linings in the production of zinc oxide. The important factor which has the impact on whole technological process includes choice of the refractory materials. The slag that remains stuck on the walls of furnace linings causes the critical states in the process of production of zinc oxide. The mechanism of degradation of the lining leads to slag rests and it is closely connected with themutual interaction of the aggressive agents with the components of the lining. Zinc melt with different chemical composition has tendency to be adhered on the surface of the lining. This process creates a new undesired surface layer which increased theoverall thickness of slag. Authors recommended a suitable refractory ceramic material for furnace aggregates and they acquired another important knowledge that can be used for modernization and effectiveness relating to the process of ind
Název v anglickém jazyce
Degradation the Refractories of Rotary Furnance Linnings in the Production of Zinc Oxide
Popis výsledku anglicky
This paper is closely connected with the complex problem of degradation relating to the refractories of rotary furnace linings in the production of zinc oxide. The important factor which has the impact on whole technological process includes choice of the refractory materials. The slag that remains stuck on the walls of furnace linings causes the critical states in the process of production of zinc oxide. The mechanism of degradation of the lining leads to slag rests and it is closely connected with themutual interaction of the aggressive agents with the components of the lining. Zinc melt with different chemical composition has tendency to be adhered on the surface of the lining. This process creates a new undesired surface layer which increased theoverall thickness of slag. Authors recommended a suitable refractory ceramic material for furnace aggregates and they acquired another important knowledge that can be used for modernization and effectiveness relating to the process of ind
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JJ - Ostatní materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
V - Vyzkumna aktivita podporovana z jinych verejnych zdroju
Ostatní
Rok uplatnění
2013
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
Sborník přednášek Hutní keramika
ISBN
978-80-87294-43-7
ISSN
—
e-ISSN
—
Počet stran výsledku
6
Strana od-do
65-70
Název nakladatele