Tribological properties of self-lubricating TiSiVN coatings at room temperature
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F68407700%3A21230%2F15%3A00229415" target="_blank" >RIV/68407700:21230/15:00229415 - isvavai.cz</a>
Výsledek na webu
<a href="http://dx.doi.org/10.1016/j.surfcoat.2014.10.016" target="_blank" >http://dx.doi.org/10.1016/j.surfcoat.2014.10.016</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.surfcoat.2014.10.016" target="_blank" >10.1016/j.surfcoat.2014.10.016</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Tribological properties of self-lubricating TiSiVN coatings at room temperature
Popis výsledku v původním jazyce
In the last years, vanadium rich coatings have been introduced as possible candidates for self-lubrication due to their optimum tribological properties. In the present investigation, the influence of V incorporation on the wear performance of TiSiN filmsdeposited onto WC substrates by d.c reactive magnetron sputtering is reported. The results achieved for TiSiVN films were compared and discussed in relation to Ti0.80Si0.15N, TiN and Ti0.82V0.15N coatings prepared as references. The tribological properties of the coatings were evaluated at room temperature on a pin on disk tribometer equipment using two different counterparts: Al2O3 and HSS balls. The wear tracks, ball-wear scars and wear debris were characterized by scanning electron microscopy with energy dispersive X-ray spectroscopy (SEM-EDS). Tribological tests indicated that the wear rate and the friction coefficient of Ti0.30Si0.15N coating decreased with continuous increase of V content being the overall behavior strongly depen
Název v anglickém jazyce
Tribological properties of self-lubricating TiSiVN coatings at room temperature
Popis výsledku anglicky
In the last years, vanadium rich coatings have been introduced as possible candidates for self-lubrication due to their optimum tribological properties. In the present investigation, the influence of V incorporation on the wear performance of TiSiN filmsdeposited onto WC substrates by d.c reactive magnetron sputtering is reported. The results achieved for TiSiVN films were compared and discussed in relation to Ti0.80Si0.15N, TiN and Ti0.82V0.15N coatings prepared as references. The tribological properties of the coatings were evaluated at room temperature on a pin on disk tribometer equipment using two different counterparts: Al2O3 and HSS balls. The wear tracks, ball-wear scars and wear debris were characterized by scanning electron microscopy with energy dispersive X-ray spectroscopy (SEM-EDS). Tribological tests indicated that the wear rate and the friction coefficient of Ti0.30Si0.15N coating decreased with continuous increase of V content being the overall behavior strongly depen
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
JK - Koroze a povrchové úpravy materiálu
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2015
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Surface & Coatings Technology
ISSN
0257-8972
e-ISSN
—
Svazek periodika
267
Číslo periodika v rámci svazku
April
Stát vydavatele periodika
NL - Nizozemsko
Počet stran výsledku
7
Strana od-do
8-14
Kód UT WoS článku
000353845700003
EID výsledku v databázi Scopus
2-s2.0-84925933059