Zatékavost polymerní taveniny v kanálech a dutině vstiřkovací formy
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F70883521%3A28110%2F05%3A63503954" target="_blank" >RIV/70883521:28110/05:63503954 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
Flow of Polymer Melts in Runners and Cavities of Injection Molds
Popis výsledku v původním jazyce
Injection molding is one of the most extended plastic processing technologies. Delivery of polymer melts into the mold cavity is the most important stage of the injection molding process. In the mold cavity the melt freezes and the product gain the finalshape and form. Plastic material does not slide along the mold surface but is instead rolled over much like rolling out a carpet. This type of laminar flow is usually described as a "fountain flow". Unusual (not expected) behaviour of polymer flow usingvarious quality of surface of spiral walls was observed. Better quality of wall surface made flow condition worse (the length of injected sample was shorter). Measurement shows that quality of surface affects on the length of flow. To verify these results it has to be made further experiments where the materials (polymers) and testing conditions will be widely changed.
Název v anglickém jazyce
Flow of Polymer Melts in Runners and Cavities of Injection Molds
Popis výsledku anglicky
Injection molding is one of the most extended plastic processing technologies. Delivery of polymer melts into the mold cavity is the most important stage of the injection molding process. In the mold cavity the melt freezes and the product gain the finalshape and form. Plastic material does not slide along the mold surface but is instead rolled over much like rolling out a carpet. This type of laminar flow is usually described as a "fountain flow". Unusual (not expected) behaviour of polymer flow usingvarious quality of surface of spiral walls was observed. Better quality of wall surface made flow condition worse (the length of injected sample was shorter). Measurement shows that quality of surface affects on the length of flow. To verify these results it has to be made further experiments where the materials (polymers) and testing conditions will be widely changed.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JQ - Strojní zařízení a nástroje
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2005
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
microCAD 2005
ISBN
963-661-658-2
ISSN
—
e-ISSN
—
Počet stran výsledku
6
Strana od-do
117-122
Název nakladatele
University of Miskolc
Místo vydání
Miskolc
Místo konání akce
Miskolc
Datum konání akce
10. 3. 2005
Typ akce podle státní příslušnosti
EUR - Evropská akce
Kód UT WoS článku
—