Úloha specifické nukleace při fotodegradaci polypropylenu
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F70883521%3A28110%2F07%3A63505287" target="_blank" >RIV/70883521:28110/07:63505287 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/61389013:_____/07:00325771
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
The Role of Specific Nucleation in Polypropylene Photodegradation
Popis výsledku v původním jazyce
The paper focuses on the effects of polymorphism on photodegradation of isotactic polypropylene. The starting polymer was modified by a specific α-nucleating agent, 1,3;2,4-bis(3,4-dimethylbenzylidene)sorbitol, by a specific β-nucleating agent,N,N'-dicyclohexylnaphthalene-2,6-dicarboxamide, or their combination. Samples prepared by compression moulding were then exposed to UV-irradiation in the interval from 0 to 240 h. The differences in morphology were reflected in different photooxidativebehaviour. Infrared spectroscopy showed that neat polypropylene was the most sensitive to photooxidation and the sample modified solely by the β-nucleating agent was the least sensitive. The remaining two samples exhibited an intermediate sensitivity. Differential scanning calorimetry revealed that the UV-exposure led to gradual changes in crystallization mechanism specifically asserting in individual materials. This behaviour was ascribed to homogeneous nucleation of partly degrad
Název v anglickém jazyce
The Role of Specific Nucleation in Polypropylene Photodegradation
Popis výsledku anglicky
The paper focuses on the effects of polymorphism on photodegradation of isotactic polypropylene. The starting polymer was modified by a specific α-nucleating agent, 1,3;2,4-bis(3,4-dimethylbenzylidene)sorbitol, by a specific β-nucleating agent,N,N'-dicyclohexylnaphthalene-2,6-dicarboxamide, or their combination. Samples prepared by compression moulding were then exposed to UV-irradiation in the interval from 0 to 240 h. The differences in morphology were reflected in different photooxidativebehaviour. Infrared spectroscopy showed that neat polypropylene was the most sensitive to photooxidation and the sample modified solely by the β-nucleating agent was the least sensitive. The remaining two samples exhibited an intermediate sensitivity. Differential scanning calorimetry revealed that the UV-exposure led to gradual changes in crystallization mechanism specifically asserting in individual materials. This behaviour was ascribed to homogeneous nucleation of partly degrad
Klasifikace
Druh
J<sub>x</sub> - Nezařazeno - Článek v odborném periodiku (Jimp, Jsc a Jost)
CEP obor
CD - Makromolekulární chemie
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GP106%2F07%2FP262" target="_blank" >GP106/07/P262: Mikrofibrilární polymer-polymer kompozity připravované in-situ</a><br>
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2007
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Polymer Degradation and Stability
ISSN
0141-3910
e-ISSN
—
Svazek periodika
—
Číslo periodika v rámci svazku
92
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
6
Strana od-do
1763-1768
Kód UT WoS článku
—
EID výsledku v databázi Scopus
—