Elektrické vlastnosti compozitů na bázi epoxy-silikonový kaučuk-carbon black
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F70883521%3A28110%2F08%3A63507374" target="_blank" >RIV/70883521:28110/08:63507374 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
PECULIARITY OF ELECTRIC PROPERTIES OF EPOXY/SILICONE RUBBER COMPOSITES FILLED WITH CARBON BLACK
Popis výsledku v původním jazyce
The specifics of electrical properties of epoxy resin/silicone rubber composites filled with carbon black in respect to their morphology and mechanical properties have been studied. There is a significant difference between percolation thresholds in composites with 25 and 50 wt. % of silicon that is attributed to the structure of such hybrid composites. When the concentration of silicon is about 25 wt. %, a multiple percolation threshold is obvious; while at 50 wt. % of silicone it is a single-stage percolation threshold. In the first case, the silicon, present in polymer blend as dispersed phase (in the form of separated non-uniform inclusions), leads to local concentration variations of carbon black per composite volume which is reflected in the composite heterogeneity increase. The rising amount of silicon up to 50 wt. % enhances the uniformity of composite from the viewpoint of its electrical response, though silicon does not form the extended phase even with so high concentration.
Název v anglickém jazyce
PECULIARITY OF ELECTRIC PROPERTIES OF EPOXY/SILICONE RUBBER COMPOSITES FILLED WITH CARBON BLACK
Popis výsledku anglicky
The specifics of electrical properties of epoxy resin/silicone rubber composites filled with carbon black in respect to their morphology and mechanical properties have been studied. There is a significant difference between percolation thresholds in composites with 25 and 50 wt. % of silicon that is attributed to the structure of such hybrid composites. When the concentration of silicon is about 25 wt. %, a multiple percolation threshold is obvious; while at 50 wt. % of silicone it is a single-stage percolation threshold. In the first case, the silicon, present in polymer blend as dispersed phase (in the form of separated non-uniform inclusions), leads to local concentration variations of carbon black per composite volume which is reflected in the composite heterogeneity increase. The rising amount of silicon up to 50 wt. % enhances the uniformity of composite from the viewpoint of its electrical response, though silicon does not form the extended phase even with so high concentration.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
JI - Kompositní materiály
OECD FORD obor
—
Návaznosti výsledku
Projekt
—
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2008
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
PPS-24 The Polymer Processing Society 24th Annual Meeting
ISBN
88-7897-025-5
ISSN
—
e-ISSN
—
Počet stran výsledku
5
Strana od-do
—
Název nakladatele
Polymer Processing Society (IT)
Místo vydání
Salerno
Místo konání akce
Salerno
Datum konání akce
19. 6. 2008
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—