On the plasma treatment of carbonyl iron particles
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F70883521%3A28110%2F10%3A63509314" target="_blank" >RIV/70883521:28110/10:63509314 - isvavai.cz</a>
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
On the plasma treatment of carbonyl iron particles
Popis výsledku v původním jazyce
Title: On the plasma treatment of carbonyl iron particles and their magnetorheology The long-term stability of magnetorheological (MR) suspensions based on carbonyl iron (CI) in silicone oil can be improved by the plasma treatment of particles surface in50% Ar + 50% octafluorcyclobutane. The X-ray photoelectron spectroscopy revealed that after 2 min of modification about 6.5% of fluorine had been bonded to the surface layer of CI particles. Subsequently, fluorine present on particles can interact withmethyl groups of silicone oil. The rheological behaviour of MR suspensions observed at the steady shear and small-strain oscillatory shear flows showed that systems on the basis of plasma-treated particles exhibit higher viscosity without magnetic fieldand thus improved long-term sedimentation stability. When the magnetic field is applied, the enhanced viscosities of suspensions caused by magnetic interactions between particles have approximately the same values irrespective of employed
Název v anglickém jazyce
On the plasma treatment of carbonyl iron particles
Popis výsledku anglicky
Title: On the plasma treatment of carbonyl iron particles and their magnetorheology The long-term stability of magnetorheological (MR) suspensions based on carbonyl iron (CI) in silicone oil can be improved by the plasma treatment of particles surface in50% Ar + 50% octafluorcyclobutane. The X-ray photoelectron spectroscopy revealed that after 2 min of modification about 6.5% of fluorine had been bonded to the surface layer of CI particles. Subsequently, fluorine present on particles can interact withmethyl groups of silicone oil. The rheological behaviour of MR suspensions observed at the steady shear and small-strain oscillatory shear flows showed that systems on the basis of plasma-treated particles exhibit higher viscosity without magnetic fieldand thus improved long-term sedimentation stability. When the magnetic field is applied, the enhanced viscosities of suspensions caused by magnetic interactions between particles have approximately the same values irrespective of employed
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
CD - Makromolekulární chemie
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/GD104%2F09%2FH080" target="_blank" >GD104/09/H080: Plazmochemické procesy a jejich technologické aplikace</a><br>
Návaznosti
Z - Vyzkumny zamer (s odkazem do CEZ)
Ostatní
Rok uplatnění
2010
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
International Conference on Advanced Plasma Technologies
ISBN
978-961-90025-9-9
ISSN
—
e-ISSN
—
Počet stran výsledku
2
Strana od-do
—
Název nakladatele
Slovenian Society for Vacuum Technique
Místo vydání
Ljubljana, Slovenia
Místo konání akce
Lake Bohinj, Slovenia
Datum konání akce
1. 1. 2010
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—