PVC Inorganic Hybrids Based on Kaolinite/Urea Intercalates
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F70883521%3A28110%2F11%3A43867234" target="_blank" >RIV/70883521:28110/11:43867234 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/70883521:28610/11:43867234
Výsledek na webu
—
DOI - Digital Object Identifier
—
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
PVC Inorganic Hybrids Based on Kaolinite/Urea Intercalates
Popis výsledku v původním jazyce
Polymer/clay hybrids materials receive much attention due to their interesting mechanical and thermal properties. Composites of poly(vinyl chloride) have been prepared by melt intercalation method using commercial type of pure kaolinite (SAK47), urea intercalated kaolinite (SAK47/urea), and intercalated/exfoliated kaolinite after washing of urea from kaolinite-urea (del. SAK47). In the next step the untreated and treated kaolinite was modified by Bis(2- ethylhexyl)phthalate, DEHP, (SAK47/DEHP, SAK47/urea/DEHP and del. SAK47/DEHP). For the PVC/kaolinite composites the suspension type of PVC with K value 60 was used. Untreated and treated kaolinite samples as well as PVC composites were examined by X-ray diffraction (XRD) and microscopy (SEM). The interactions between kaolinite and modifier were discussed by FTIR-ATR. Tested mechanical properties were improved almost for all PVC mixtures. The highest values of tensile strength and E-modulus were observed for PVC+del.SAK47/DEHP.
Název v anglickém jazyce
PVC Inorganic Hybrids Based on Kaolinite/Urea Intercalates
Popis výsledku anglicky
Polymer/clay hybrids materials receive much attention due to their interesting mechanical and thermal properties. Composites of poly(vinyl chloride) have been prepared by melt intercalation method using commercial type of pure kaolinite (SAK47), urea intercalated kaolinite (SAK47/urea), and intercalated/exfoliated kaolinite after washing of urea from kaolinite-urea (del. SAK47). In the next step the untreated and treated kaolinite was modified by Bis(2- ethylhexyl)phthalate, DEHP, (SAK47/DEHP, SAK47/urea/DEHP and del. SAK47/DEHP). For the PVC/kaolinite composites the suspension type of PVC with K value 60 was used. Untreated and treated kaolinite samples as well as PVC composites were examined by X-ray diffraction (XRD) and microscopy (SEM). The interactions between kaolinite and modifier were discussed by FTIR-ATR. Tested mechanical properties were improved almost for all PVC mixtures. The highest values of tensile strength and E-modulus were observed for PVC+del.SAK47/DEHP.
Klasifikace
Druh
D - Stať ve sborníku
CEP obor
CD - Makromolekulární chemie
OECD FORD obor
—
Návaznosti výsledku
Projekt
<a href="/cs/project/ED2.1.00%2F03.0111" target="_blank" >ED2.1.00/03.0111: Centrum polymerních systémů</a><br>
Návaznosti
P - Projekt vyzkumu a vyvoje financovany z verejnych zdroju (s odkazem do CEP)<br>Z - Vyzkumny zamer (s odkazem do CEZ)<br>S - Specificky vyzkum na vysokych skolach
Ostatní
Rok uplatnění
2011
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název statě ve sborníku
NetWare2011
ISBN
978-1-61208-151-9
ISSN
—
e-ISSN
—
Počet stran výsledku
5
Strana od-do
109-113
Název nakladatele
IARIA
Místo vydání
US
Místo konání akce
Nice/Saint Laurent du Var, France
Datum konání akce
21. 8. 2011
Typ akce podle státní příslušnosti
WRD - Celosvětová akce
Kód UT WoS článku
—