RheoTack evaluation of detaching behavior of silicone-based pressure sensitive adhesives for transdermal therapeutic systems
Identifikátory výsledku
Kód výsledku v IS VaVaI
<a href="https://www.isvavai.cz/riv?ss=detail&h=RIV%2F70883521%3A28110%2F25%3A63594740" target="_blank" >RIV/70883521:28110/25:63594740 - isvavai.cz</a>
Nalezeny alternativní kódy
RIV/70883521:28610/25:63594740
Výsledek na webu
<a href="https://www.sciencedirect.com/science/article/pii/S026322412500795X?via%3Dihub" target="_blank" >https://www.sciencedirect.com/science/article/pii/S026322412500795X?via%3Dihub</a>
DOI - Digital Object Identifier
<a href="http://dx.doi.org/10.1016/j.measurement.2025.117436" target="_blank" >10.1016/j.measurement.2025.117436</a>
Alternativní jazyky
Jazyk výsledku
angličtina
Název v původním jazyce
RheoTack evaluation of detaching behavior of silicone-based pressure sensitive adhesives for transdermal therapeutic systems
Popis výsledku v původním jazyce
This study focuses on applying the RheoTack method to assess the detaching behavior of transdermal therapeutic systems (TTS), which represent skin-applied medications comprising a drug-loaded pressure-sensitive adhesive (PSA) and a flexible backing layer. The RheoTack method provides detailed force-retraction displacement-curves (F-h-curves) that reveal the influence of chemical structure and resin content on PSA deformation and fibril formation. To compare various rod geometries (flat rods with diameters of 5 mm and 8 mm, and a spherically rounded rod with a contact area of 5 mm2), the force-retraction displacement curves were normalized to account for the effective contact areas. The flat and spherical rods led to completely different F-h-curves as well as different failure and tack behaviors. Furthermore, the adhesion formation between the TTS with flexible backing layers and rods during the dwell phase occurs in a different manner compared with rigid plates, particularly for flat rods, where maximum compression stresses occur at the edges and not uniformly over the cross-section. Measurements of F-h-curves were performed with retraction speeds of 0.01, 0.1, and 1 mm/s. The increase in retraction speed increased the stiffness from 250 to 1200 N/m for non-amine-compatible PSA measured with a rod of 8 mm. RheoTack measurements were performed with a dwell time of 1 s, which is consistent with ASTM D2949. However, the TTS was in the adhesion-establishing compression phase for 3 s at 1 mm/s and for 30 s at 0.01 mm/s. Thus, the approach to follow ASTM D2949 has to be reconsidered for testing TTS materials.
Název v anglickém jazyce
RheoTack evaluation of detaching behavior of silicone-based pressure sensitive adhesives for transdermal therapeutic systems
Popis výsledku anglicky
This study focuses on applying the RheoTack method to assess the detaching behavior of transdermal therapeutic systems (TTS), which represent skin-applied medications comprising a drug-loaded pressure-sensitive adhesive (PSA) and a flexible backing layer. The RheoTack method provides detailed force-retraction displacement-curves (F-h-curves) that reveal the influence of chemical structure and resin content on PSA deformation and fibril formation. To compare various rod geometries (flat rods with diameters of 5 mm and 8 mm, and a spherically rounded rod with a contact area of 5 mm2), the force-retraction displacement curves were normalized to account for the effective contact areas. The flat and spherical rods led to completely different F-h-curves as well as different failure and tack behaviors. Furthermore, the adhesion formation between the TTS with flexible backing layers and rods during the dwell phase occurs in a different manner compared with rigid plates, particularly for flat rods, where maximum compression stresses occur at the edges and not uniformly over the cross-section. Measurements of F-h-curves were performed with retraction speeds of 0.01, 0.1, and 1 mm/s. The increase in retraction speed increased the stiffness from 250 to 1200 N/m for non-amine-compatible PSA measured with a rod of 8 mm. RheoTack measurements were performed with a dwell time of 1 s, which is consistent with ASTM D2949. However, the TTS was in the adhesion-establishing compression phase for 3 s at 1 mm/s and for 30 s at 0.01 mm/s. Thus, the approach to follow ASTM D2949 has to be reconsidered for testing TTS materials.
Klasifikace
Druh
J<sub>imp</sub> - Článek v periodiku v databázi Web of Science
CEP obor
—
OECD FORD obor
20302 - Applied mechanics
Návaznosti výsledku
Projekt
—
Návaznosti
I - Institucionalni podpora na dlouhodoby koncepcni rozvoj vyzkumne organizace
Ostatní
Rok uplatnění
2025
Kód důvěrnosti údajů
S - Úplné a pravdivé údaje o projektu nepodléhají ochraně podle zvláštních právních předpisů
Údaje specifické pro druh výsledku
Název periodika
Measurement
ISSN
0263-2241
e-ISSN
—
Svazek periodika
253
Číslo periodika v rámci svazku
Part A
Stát vydavatele periodika
GB - Spojené království Velké Británie a Severního Irska
Počet stran výsledku
13
Strana od-do
nestránkováno
Kód UT WoS článku
001463102300001
EID výsledku v databázi Scopus
2-s2.0-105001736708